Lead-free SMT Soldering Defects How to Prevent Them
Published: |
October 23, 2012 |
Author: |
Peter Biocca, Senior Development Engineer |
Abstract: |
Tin-Silver-Copper alloys are the primary choice for lead-free SMT assembly. Although there are other options available such as alloys containing bismuth or indium and other elements, tin-silver-copper solders, also known as SAC alloys are by far the most popular. They are used by approximately 65% of users, as last surveyed by Soldertec in 2003.... |
You must be a registered user to talk back to us. |
Company Information:
- Jul 20, 2017 - Reactivity Of No-Clean Flux Residues Trapped Under Bottom Terminated Components
- May 17, 2017 - How to Use the Right Flux for the Selective Soldering Application
- Dec 29, 2016 - Partially-Activated Flux Residue Impacts on Electronic Assembly Reliabilities
- Feb 13, 2009 - SnCu Based Alloy Design for Lower Copper Dissolution and Better Process Control
- Jan 15, 2009 - Creating Solder Joint Reliability with SnCu Based Solders Some Practical Experiences
- See all SMT / PCB technical articles from Kester »
More SMT / PCB assembly technical articles »
- Mar 19, 2024 - What is Underfill | GPD Global
- Mar 19, 2024 - Made in Japan: Solder Paste Jet Dispensing Machine | I.C.T ( Dongguan ICT Technology Co., Ltd. )
- Feb 26, 2024 - Precision Control in Electronic Assembly: Selective Wave Soldering Machine | I.C.T ( Dongguan ICT Technology Co., Ltd. )
- Feb 02, 2024 - Maximizing Efficiency: The High-Speed SMT Line With Laser Depanelizer | I.C.T ( Dongguan ICT Technology Co., Ltd. )
- Dec 27, 2023 - Revolutionizing Tech: SMT Auto IC Programming Machine Mastery | I.C.T ( Dongguan ICT Technology Co., Ltd. )
- Browse Technical Library »
Lead-free SMT Soldering Defects How to Prevent Them article has been viewed 1088 times