Fill the Void V - Mitigation of Voiding for Bottom Terminated Components

Published:

December 29, 2020

Author:

Tony Lentz, FCT Assembly & Greg Smith, BlueRing Stencils

Abstract:

Voiding in solder joints has been studied extensively, and the effects of many variables compared and contrasted with respect to voiding performance. Solder paste flux, solder powder size, stencil design, circuit board design, via-in-pad design, surface finish, component size, reflow profile, vacuum reflow, nitrogen reflow and other parameters have been varied and voiding quantified for each. The results show some differences in voiding performance with respect to most of these variables but these variables are not independent of each other. Voiding in solder joints is a complex issue that often requires multiple approaches to reduce voiding below required limits. This paper focuses on solutions to voiding for commonly used bottom terminated components (BTCs)....

  • Download Fill the Void V - Mitigation of Voiding for Bottom Terminated Components article
  • To read this article you need to have Adobe PDF installed

You must be a registered user to talk back to us.

 
Company Information:

FCT ASSEMBLY, INC.

With numerous facilities in the United States, we are one of the electronics industry's leading manufacturers of lead-free solder products, superior quality stencils, and precision cut parts.

Greeley, Colorado, USA

Manufacturer of Assembly Material, Soldering

  • Phone 970-346-8002
  • Fax 970-346-8331

FCT ASSEMBLY, INC. website

Company Postings:

(14) products in the catalog

(13) technical library articles

(176) news releases

  • Dec 07, 2020 - A Non-destructive Approach to Identify Intermittent Failure Locations on Printed Circuit Cards (PCC) that have been Temperature Cycle Tested | ACI Technologies, Inc.
  • Dec 02, 2020 - SMT007-MIRTEC Intelligent Factory Automation Article-November 2020 | MIRTEC Corp
  • Nov 09, 2020 - Ball Grid Array (BGA) Voiding Affecting Functionality | ACI Technologies, Inc.
  • Nov 04, 2020 - WHY CLEAN A NO-CLEAN FLUX | KYZEN Corporation
  • Nov 04, 2020 - Higher Defluxing Temperature and Low Standoff Component Cleaning - A Connection? | ZESTRON Americas
  • Browse Technical Library »

Fill the Void V - Mitigation of Voiding for Bottom Terminated Components article has been viewed 142 times

Your 2021 Eptac IPC Training Schedule

fluid dispensing pumps for integration