Electronics Forum: pcb baking (Page 7 of 35)

Bakeing

Electronics Forum | Mon Nov 20 06:51:00 EST 2000 | Daniel Carlsson

Does anyone have information regarding: -Moisture level (wt%) that may cause delamination in PCB�s. -Baking time and temperature if using a Vacuum Drying Cabinett and if using an air oven. (What I�m most interested of is Poly-Imid-Aramid.) -Are ther

Reflow soldering issue

Electronics Forum | Thu Aug 30 16:17:07 EDT 2018 | emeto

First suspect PCB contamination - clean the boards, bake/dry them, try again.

Re: Wash and bake of blank PCB's before assembly

Electronics Forum | Thu Feb 12 17:21:07 EST 1998 | Justin Medernach

| I would appreciate any information concerning the wash and bake of blank Printed Circuit Boards | before assembly. | + Is it necessary to wash and bake PCB�s before assembly? | + If any, what is the reason for wash and bake of PCB�s? | + If any, wh

Solder voids in PTH

Electronics Forum | Wed Feb 20 09:29:19 EST 2008 | mun4o

ni, I had similar problem too.I bake PCB in SW mashine - about 8h ,T=90 C.Problem is in the base material of PCB - there are moisture in the material.After my complaint to PCB factory , they change material and the problem disappear.

Immersion silver life span

Electronics Forum | Wed Apr 13 05:48:52 EDT 2005 | charly

hi' i need advise on immersion silver PCb shelf life. 1) what is the shelf life for Immersion silver PCB? 2) iF PCB expire, can we bake the immersion PCB? what temp & duration? 3) How long can we keep the pCB again after rebaking? (with vacuum seal)

Flex-rigid PCB

Electronics Forum | Wed Jun 24 18:50:31 EDT 2020 | premkumar_haribabu

Dear experts, We are in stage to fix lapse or hold time between pre-bake to reflow process ( SMT ) for flex-rigid PCB, usually for flex pcb , we need to assemble as early as possible once after baking & if not , we can store in humidifier up to some

Baking assemblies after ultrasonic water wash

Electronics Forum | Thu Jun 11 22:57:45 EDT 2009 | davef

NASA recommends baking a PCB for a minimum of 4 hours at 93+/- 5.5�C before conformally coating. [NASA-STD-8739.1, �Workmanship Standard for Staking and Conformal Coating of Printed Wiring Boards and Electronic Assemblies,� August 6, 1999]

HIC turn Pink for PCB-URGENT

Electronics Forum | Tue Jul 06 05:33:46 EDT 2004 | ANDREW

1)What is the MSD level for PCB? 2)I have some PCB's with HIC (humidity indicator card ) has turn to pink at 50%. Should I bake the PCB prior to assembly process.This fab is a complex board with various kind advance package assembled on the board.

Re: Baking Components ?

Electronics Forum | Fri Jul 30 17:26:02 EDT 1999 | John Thorup

| | Surface Mount Components like QFP's in Tray usually comes sealed in an anti-static plastic pack. In case the QFP's were removed from the said anti-static bag for more than 2 weeks, do these components needed to be baked for they might produce so

Flux residue cleaning procedure

Electronics Forum | Tue Oct 31 01:32:47 EST 2006 | hanocete

thanks for your reply, actually we bake the PCB assembly prior the rework because the package was exposed for quite some time already. The baking time was 24hrs @ 125 deg.C. We notice that there were flux residues on the connectors after the baking.


pcb baking searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830