BGA PROCESS MATERIAL

Electronics Forum | Fri Feb 20 08:56:42 EST 2004 | davef

We successfully clean WS flux on 1mm and 1.25mm pitch BGA. For 0.8mm pitch BGA, we use no clean, because we cannot remove the flux residue from under them efficiently. Use ion chromatography testing to be sure it is clean under the BGA. IC is the on

changing from no-clean to clean

Electronics Forum | Tue May 21 17:16:51 EDT 2002 | davef

Larry, Yes, no matter how much you�d like to avoid using NC, you probably will have to start using the stuff, if the design [sales, in your case] types have their way. We can clean WS under 1mm and 1.25mm pitch BGA. For 0.8mm pitch BGA, we use NC.

0402 stencil design

Electronics Forum | Tue Feb 04 22:28:16 EST 2003 | davef

You could reduce the paste by about 70%. Solder balling and tombstoning will be the issues to fight. The drivers to these don't change with the component size. Use the fine SMTnet Archives for background. Aperture Size and Thickness of Solder Pas