Electronics Forum | Fri Feb 18 15:27:38 EST 2005 | jluckenbaugh
Frank R, I believe the Dymax #984-LVUF is a POLYURETHANE RESIN. I have used Humiseal 1A27 and 1A33 for several years with great success. Both of these materials are High VOC materials. If your customer does not require these materials to be aproved
Electronics Forum | Wed Mar 04 08:32:45 EST 2020 | stephendo
We bought a conformal coating removal machine AKA a sand blaster at an auction. It is a CCR2000 especially made to be ESD safe. Does anyone have any experience with sandblasting conformal coating? We mostly use humiseal 1A33 and UV40. When we use the
Electronics Forum | Fri Feb 18 12:00:08 EST 2011 | dennisfo
That has also been the standard here. We have a urethane line which pulls a vacuum on the mixture before transfering to the can. I plan on testing this out before receipt of the 73 thinner. I've also received some feedback with indication that the mi
Electronics Forum | Tue Mar 01 15:07:00 EST 2011 | dennisfo
Update on 1B73 bubbles, Changed over to a mixture of Humiseal 73 thinner with coating (25 sec on Zahn 2) observed a reduction in bubble formation (approx. 20%) but still present.
Electronics Forum | Tue Mar 01 15:33:35 EST 2011 | jlawson
If I assume you running a selective coating machine ? Maybe you have small leak and system is sucking in air creating bubbles in mixture, like a sort of venturi action, just idea, can be a faulty fitting , elbow etc. Have had this before....
Electronics Forum | Tue Feb 08 14:23:47 EST 2011 | dennisfo
Conformal coat bubbles using 1B73 and SC-205 nozzle I've read most of the posts on this subject. I'm using the SC-205 (airless) fan nozzle and 400 needle to apply 1B73 mixed with xylene thinner. I have micro bubbles which come directly out of the noz
Electronics Forum | Wed Feb 16 12:47:58 EST 2011 | dennisfo
I've been here approx. 3 months. It was indicated that Xylene has alwas been used but it was never indicated that bubbles were not present in the past (ignored or touchup). I have a sample of Humiseal 73 thinner ordered for testing. We've been thinne
Electronics Forum | Mon Aug 20 09:49:57 EDT 2018 | dontfeedphils
Not entirely clear on your question. We don't coat any of our hardware (assemblies are coated prior to hardware installation), so if coating needs to be reworked after this, then hardware removal is needed.
Electronics Forum | Sat Aug 18 10:35:41 EDT 2018 | mgerrior
Hey Phil, i'm just curious what your rework processes are for your hardware after conformal coating is applied (if any). I'm interested in conformal coating as our hardware can be exposed to moisture rich environments at customer sites but to my kno
Electronics Forum | Tue Jul 03 01:54:42 EDT 2018 | rdhiman1
Reaching out to all conformal coating experts, please help! While setting up conformal coating using the automated atomized spray, we observing issues associated with conformal coating wetting on the following regions: 1) Component edges 2) Metalli