Electronics Forum | Tue Feb 24 09:47:45 EST 2015 | rgduval
Well, since you're looking at a water soluble flux from AIM, I'm guessing you wash the boards before you conformal coat them. Thus, I wouldn't expect any interaction between the excess flux that you're washing off of the boards and the Humiseal that
Electronics Forum | Wed Jan 31 10:56:23 EST 2018 | dontfeedphils
I'm working on bringing up a new conformal coat process/workcenter and have a few questions I'm hoping someone might have experience with. Right now we're manually spraying both coating materials (1B31 and 1A33 from Humiseal) using HVLP guns. I run
Electronics Forum | Tue Jul 31 10:16:59 EDT 2012 | silverbullet
We are in the process of revamping our conformal coating room. Presently, we have a C-740 Nordson Asymtek coating machine that sprays most of our boards with Dow Corning 2577. We are spending a lot of time masking boards and are thinking of upgrading