Electronics Forum | Tue Jan 20 06:46:39 EST 1998 | IgmarG
This is a re-post of my previous message. I typed my Email address wrong in the other message. I am sorry for any inconvenience caused. Is there anyone who can tell me what is the maximum allowable soldering temperature when soldering a TQFP (Thin Qu
Electronics Forum | Thu Jan 29 08:33:34 EST 1998 | Mike Moninger
| This is a re-post of my previous message. I typed my Email address wrong in the other message. I am sorry for any inconvenience caused. | Is there anyone who can tell me what is the maximum allowable soldering temperature when soldering a TQFP (Thi
Electronics Forum | Wed Jan 21 22:35:01 EST 1998 | Scott
| Is there anyone who can tell me what is the maximum allowable soldering temperature when soldering a TQFP (Thin Quad Flat Pack) device in a reflow oven? We recently used a CY7C375i in a TQFP160 package and we experienced warping (bending) of this c
Electronics Forum | Tue Apr 13 09:11:54 EDT 1999 | Dave F
| We process both tin/lead plated boards and gold plated boards in our surface mount group. I have used Sn62/Pb36/Ag2 solder paste on all gold plated boards to help prevent gold scavaging. To reduce the amount of different solder pastes we have to
Electronics Forum | Mon Apr 19 02:45:31 EDT 1999 | Brian Sloth Bentzen
| | We process both tin/lead plated boards and gold plated boards in our surface mount group. I have used Sn62/Pb36/Ag2 solder paste on all gold plated boards to help prevent gold scavaging. To reduce the amount of different solder pastes we have t
Electronics Forum | Tue Apr 17 09:38:04 EDT 2001 | CAL
With some help from our good Friends at Agilent Technologies our RF Lab includes testing up to 100GHz. Equipment includes Vector network analyzer, signal analyzer, dual channel power meter, noise filter meter, advanced impedance analyzer (including
Electronics Forum | Tue Apr 13 17:44:29 EDT 1999 | Christopher Lampron
| We process both tin/lead plated boards and gold plated boards in our surface mount group. I have used Sn62/Pb36/Ag2 solder paste on all gold plated boards to help prevent gold scavaging. To reduce the amount of different solder pastes we have to
Electronics Forum | Thu Apr 22 17:19:57 EDT 1999 | JohnW
| | We process both tin/lead plated boards and gold plated boards in our surface mount group. I have used Sn62/Pb36/Ag2 solder paste on all gold plated boards to help prevent gold scavaging. To reduce the amount of different solder pastes we have t
Electronics Forum | Thu Sep 10 21:48:37 EDT 1998 | Dave F
| I'm very familiar with the great board space savings of BGA and all the "claims to fame." However, can someone out there tell me if any concern exist in the inspection realm. Additionally, solder cracking, CTE/TCE mismatches, no leads for stress re
Electronics Forum | Tue May 04 10:30:35 EDT 1999 | Dave F
| I am about to embark on an effort to evaluate 3 different solder material suppliers and their recommended materials for our assembly process, in an effort to find the best supplier/material. We do mixed technology, with NOCLEAN chemistry so I will