Electronics Forum | Wed Jun 04 09:15:06 EDT 2003 | davef

We used to use 260+-5C (500+-10F) for Sn63, now we use 240-260C (460-480 F). You probably could get away with 232C (450F) in all cases, since there is no thermal mass to a lead being tinned. We keep our tinning temperature the same as our solder po

Circuit Card Assembly Molding

Electronics Forum | Fri Apr 01 17:45:31 EDT 2011 | smt_guy

thanks for all your replies. we tried running our beta runs and have lots of issues. first our molding process which was set to 450'F temp at 1200 PSI smashed the circuit card components and penetrated the epoxy compound we used to encapsulate the C

Reflow Oven Chain Lubrication

Electronics Forum | Wed Oct 23 16:56:03 EDT 2002 | mikestringer

Hi Marc I too have been using a fully synthetic Motor oil on Heller reflow ovens for a number of years. In our case Mobil 1 5W-50. We have a field failure problem with some 1% resistors under conformal coating where sulphates are dissolving the si