Electronics Forum | Mon Mar 05 17:19:38 EST 2007 | bman
I've wondered about the 5% spec myself. Section 4.2 points out that "The oven used for baking shall be vented and capable of maintaining the required temperature at less then 5% RH.", leading me to believe this spec even applies to ovens used to bak
Electronics Forum | Wed Jul 03 11:37:36 EDT 2002 | fmonette
Dason, I apologize if some of the information sounds redundant but I don't think I explained my point very well (and the standard can get really confusing at times). I definitely agree with using C-SAM to look for internal defects. My only advise i
Electronics Forum | Tue Apr 13 14:49:15 EDT 2010 | davef
90%) from the sample, and the bake time and temperature specified herein are minimums. To improve test accuracy, or to prevent heat damage, other bake parameters may be AABUS. 2 Applicable Documents IPC-QL-653 Certification of Facilities that Inspect
Electronics Forum | Wed Sep 29 04:30:27 EDT 1999 | ROBERT
| | Hi All, | | Any one experince BGA-chipset warp about 10-15mil after removing | | from PCB? | | FYI, the rework temperature for preheat was 170C from room | | temperature about 30 seconds, & BGA was removed at temperature | | between 190-200C.
Electronics Forum | Fri Oct 04 11:34:42 EDT 2002 | Bob Willis
Some additional comments from a paper may be of interest. Baking Printed Circuit Boards - Why and How Baking printed boards prior to conventional and surface mount assembly should not be necessary. Often boards are baked for historical reasons; in
Electronics Forum | Mon Mar 22 07:35:41 EST 2004 | Chris Lampron
We too are baking required components at 125 degrees C. One of the problems that is comming up is components packaged in tubes. The tubes cannot stand the 125 degree requirement without melting. 50 degrees is a safe temperature for low temp carriers
Electronics Forum | Fri Aug 24 17:30:40 EDT 2007 | jmelson
Oh, for a second there I thought it was 257 C, not F. Solder temperature! Still, one WEEK at 257 F seems way extreme. Maybe this is to bake out a part that has been underwater for a week. Is this a military part? I can't imagine any commercial-g
Electronics Forum | Mon Oct 11 14:01:25 EDT 2010 | clampron
Good Afternoon, The PVC tubes, unless marked otherwise, cannot see 125 degrees C. I have baked smaller level 3 parts at 40 degrees C for 9 days in the tube. I had tried several different temperatures but found out the the max temp for the tubes is d
Electronics Forum | Wed Apr 26 06:09:12 EDT 2017 | ajaytyagi
Hi, Pl let me know about opinion/experience whether thick film chip SMD resistor which is MSL-1 Required to bake before being usedon SMT line. I want to use SMD resistance spool which is around 2 yeasr old kept at 25 deg room temperature at around 4
Electronics Forum | Fri Jul 30 17:16:59 EDT 1999 | Dave F
| Hello Netters, | | I have a customer who wants us to aquaeos wash a PCB after all operations have been performed. The PWB is two layer FR4 with a Transformer, a Multichip Module with Conformal Coating, (6) 11" insulated wires that are tinned on e