Electronics Forum | Tue Apr 23 18:34:45 EDT 2002 | mkallen
My first posting was not very clear -- sorry. Let me try again. What I want to know is: can I eliminate the drying (baking) process completely IF I know that the good parts (i.e., those not being reworked) are going to stay under some threshold tem
Electronics Forum | Thu Apr 25 09:34:24 EDT 2002 | fmonette
Michael, By the way, the default bake duration should be 48 hours at 125C instead of 24 hours. The shorter duration was based on a standard that is now obsolete. The current revision of J-STD-033 includes a variable duration bake table, based on co
Electronics Forum | Thu Feb 07 09:07:10 EST 2002 | fmonette
Dason, Please be aware that weight gain is only a very crude estimate of the component moisture content. This is only accurate when the moisture is uniformly distributed inside the component (which is actually never). This measurement is usually no
Electronics Forum | Fri Nov 05 21:22:34 EST 1999 | chartrain
Amazing in today's technology that people still bake because "that's the way we've alawys done it". Baking is a band aid for poor manufacturing of the PCB. Moisture can become trapped between the layers during buildup. This moisture when it contacts
Electronics Forum | Thu Feb 12 17:21:07 EST 1998 | Justin Medernach
| I would appreciate any information concerning the wash and bake of blank Printed Circuit Boards | before assembly. | + Is it necessary to wash and bake PCB�s before assembly? | + If any, what is the reason for wash and bake of PCB�s? | + If any, wh
Electronics Forum | Thu Aug 05 16:15:18 EDT 2004 | pjc
Are you considering baking due to moisture exposure? Not all OSPs are created equal. I would check with your PWB fabricator about dry times and effects on their OSP finish. After you get it, I'd still try just one PWB for bake-dry out and check solde
Electronics Forum | Mon Aug 25 12:18:10 EDT 2008 | evtimov
I am looking for an inexpensive way to bake just > a few components. would a toaster oven be okay on > the low setting (i would get a thermometer!) do i > need to get something to place the components on? > maybe a silicon cooking mat (not sure a
Electronics Forum | Fri Apr 23 17:59:54 EDT 2010 | hegemon
Therein lies the issue. Unknown storage conditions before we received the PCBs, date codes just expired (2 weeks), first article is de-lam city! Had a bad feeling about it. Have read some studies showing that there is no linear tie in of visual cha
Electronics Forum | Thu Jan 26 14:47:46 EST 2006 | james
Just wondering what others are doing as far MSD parts. We keep most of our parts in the dry cabinet before use. Most bags are openend and have passed the recomendation as far as mounting within a certain time. We have had defects with boards that
Electronics Forum | Thu Aug 24 15:54:13 EDT 2006 | davef
It depends. What is: * Storage environment and period * Board laminate, epoxy, and copper thickness of PTH * Down stream process * Etc FR4 0.062" thick boards absorb between 0.08 to 0.1%Wt of moisture within a 24 hour period, and 0.2 to 0.23%Wt in