component baking

Electronics Forum | Fri Aug 16 17:08:07 EDT 2002 | davef

Could be. It does indicate imperfection. * �The component was manufactured and shipped correctly and should not need baking in order to use it.� => Sounds good. Most classes of MSD packaging have a self-life. Lots of times it�s expired before it

BGA baking

Electronics Forum | Sun Mar 20 14:47:29 EDT 2011 | floydf

We are going to be placing BGAs for the first time, and I have some questions. Is it recommended top bake all of the boards and all of the BGAs before production? I have had good luck baking boards that didn't wave solder well. It usually turns out

baking out pcbs after reflow process

Electronics Forum | Fri Jul 13 08:03:54 EDT 2012 | cobham1

I appreciate all the feedback. The reason I was asking the question is because we have an internal documnet that states we need to bake for 16 hours after the boards are cleaned. This just seemed to long for what little moisture is really removed. I

baking out pcbs after reflow process

Electronics Forum | Thu Jul 05 11:26:08 EDT 2012 | cobham1

I need help with how long do I need to bake out double sided PCB's that have been cleaned. The units will not be reworked but instead will be moved on to hand stuffing. I have looked in IPC CH-65B and J-STD-033C. I get information for parts if I am r

MSL Project

Electronics Forum | Fri Mar 09 04:10:18 EST 2012 | grahamcooper22

Hi, I've been supplying Totech dry cabinets in the Uk for 10 years and in that time I've realised the only places to find the correct MSL level is on the dry pack the devices are shipped in or by spending hours on the internet or speaking to the devi

baking PWB standard??

Electronics Forum | Tue Aug 26 07:44:06 EDT 2008 | davef

Industry-wide, there is no current requirement for baking of bare boards. It adds no value. * IPC-HDBK-001 has guidelines olden times. * IPC-TM-650 has several test methods to determine moisture resistance to both liquid immersion and absorption from

Baking Components - query

Electronics Forum | Mon Oct 11 14:01:25 EDT 2010 | clampron

Good Afternoon, The PVC tubes, unless marked otherwise, cannot see 125 degrees C. I have baked smaller level 3 parts at 40 degrees C for 9 days in the tube. I had tried several different temperatures but found out the the max temp for the tubes is d

baking out pcbs after reflow process

Electronics Forum | Fri Jul 06 10:35:32 EDT 2012 | ashworth14

All i used to do was blow them with an airline to remove the excess moisture then bake them for 15/20 min at 100' in an oven and that seems to work fine, i did get the info from a 4 stage cleaning guide for the actual cleaning solution we used but it

Need Help for CCGA Rework

Electronics Forum | Tue Nov 01 15:26:43 EST 2005 | GS

Is it this your first experience of C-CGA RWK ? In order to approach a RWK of this kind of pakage it requires a capable process and clear operating procedure. In the past, the company who I use to work for, we rwkd plenty of this kind of CCGA. Earl

Make That F

Electronics Forum | Fri Jul 30 17:24:24 EDT 1999 | Dave F

| | Hello Netters, | | | | I have a customer who wants us to aquaeos wash a PCB after all operations have been performed. The PWB is two layer FR4 with a Transformer, a Multichip Module with Conformal Coating, (6) 11" insulated wires that are tinne


bake time searches for Companies, Equipment, Machines, Suppliers & Information

PCB Handling with CE

World's Best Reflow Oven Customizable for Unique Applications
SMTAI 2024 - SMTA International

Stencil Printing 101 Training Course
2024 Eptac IPC Certification Training Schedule

High Precision Fluid Dispensers
2024 Eptac IPC Certification Training Schedule

Software for SMT placement & AOI - Free Download.
PCB Depanelizers

Private label coffee for your company - your logo & message on each bag!