Electronics Forum | Wed Dec 03 07:30:57 EST 2008 | realchunks
Hi System Steve, What is a solvent cleaner over water wash? Solvent first and then rinse with water? And why do they feel the need to bake the boards? Do they think trapped moisture will cause board damage?
Electronics Forum | Tue Oct 30 21:42:32 EST 2001 | surachai
I have question about board baking after in line washing machine then I would like to know some information that ; 1) Do we need board baking after in line washing machine? Both bare board and assembly borad normally we don't bake . 2)In case of ne
Electronics Forum | Fri May 15 17:31:04 EDT 1998 | Steve Abrahamson
| | | | We had some failures on an IC package that the manufacturer has put down to moisture inside the package, leading to popcorning. | | | | This seems a bit odd, the package is a PLCC 84 which is quite thick. I have only seen this problem on thin
Electronics Forum | Wed Dec 03 08:39:09 EST 2008 | sys_steven
boards are polyimide, and it is an ipa rinse with the solvent cleaner.
Electronics Forum | Tue Dec 02 18:10:39 EST 2008 | sys_steven
Need your opinion guys.. The old timers at the plant here feel that we should clean our board after Misprints withe the solvent cleaner over water wash. This is so they don't have to rebake the pcb for 24 hours before smt again. I don't believe th
Electronics Forum | Fri Jul 30 17:16:59 EDT 1999 | Dave F
| Hello Netters, | | I have a customer who wants us to aquaeos wash a PCB after all operations have been performed. The PWB is two layer FR4 with a Transformer, a Multichip Module with Conformal Coating, (6) 11" insulated wires that are tinned on e
Electronics Forum | Tue Dec 09 10:04:36 EST 2008 | lazzara55
SMT-ypw: Does PWB supplier start to implement PWB drying packaging? B3: YES! The fabrication of the PCB involves a series of wet processing that requires counter-measures to remove moisure. While some of the PCB processes also include bake cycles th
Electronics Forum | Thu Dec 04 00:22:11 EST 2008 | maacolomer
Hi Steven, The 24 hrs bake is an overkill according with various J-STDs. Assuming a bake temperature over the 100 Celsius degrees. There are several factors to be considered before deciding the best methodology to wash misprinted board. However,
Electronics Forum | Fri Jul 30 17:24:24 EDT 1999 | Dave F
| | Hello Netters, | | | | I have a customer who wants us to aquaeos wash a PCB after all operations have been performed. The PWB is two layer FR4 with a Transformer, a Multichip Module with Conformal Coating, (6) 11" insulated wires that are tinne
Electronics Forum | Wed Dec 19 02:24:40 EST 2001 | ianchan
Did I mention, we tried to use the same WS flux formulae to brush-cover the affected flex-PCB pads, and subject it to another round of water-wash, followed by oven-baking, and it still doesn't help abit? Oven bake : 100 deg-C, approx 15~30mins (manu
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830