Re: Is baking PCB necessary before solder process?

Electronics Forum | Thu Jul 29 12:33:38 EDT 1999 | Wolfgang Busko

| Currently, we are baking any PCB before process on SMT, the 'reason' is to dry any possible humidity that could be inner the PCB, it does not matter if the PCB is multilayer or not. We bake PCB's at 107C for 4 hrs and the board must be process into

pcb physical handling

Electronics Forum | Wed May 04 10:42:55 EDT 2005 | nice90

Handling a PCB 1. Check your ESD slippers and ESD Strap first before entering the SMT production line 2. A PCB manufactred over 90 days must be stored first on the baking Oven before Production 3. Temperature on the Baking oven must be 125plus and m

defects in pcb manufacturing

Electronics Forum | Wed Oct 28 09:28:02 EDT 2009 | spitkis2

I agree with you. Personally, I would either return them and look for a new supplier or scrap these boards. Unless your customer provided these boards and gave you the go ahead to populate them, they will not be too pleased about the build.

Floor life pcb assembly

Electronics Forum | Wed Apr 23 19:00:39 EDT 2008 | stevek

It depends on the laminate but a PWB is like any other MSL component. Some fab shops are only waranting standard FR4 laminates for 45-60 days when processed at lead free temperatures. The best thing I can say is to try some weight gain/loss experim

seperation of soldermask and pcb

Electronics Forum | Tue Mar 25 09:35:28 EDT 2014 | emeto

Have you tried to bake the boards before you process them?

seperation of soldermask and pcb

Electronics Forum | Tue Mar 25 10:31:05 EDT 2014 | sara_pcb

The boards are baked for 2 hours at 120 deg C Regards, R.Saravanan

0.031 pcb bowing -- solutions?

Electronics Forum | Tue Aug 28 08:28:30 EDT 2012 | rgduval

We agree with all of the previous comments, and would add the following: Warpage is generally caused by excess moisture in the raw boards. Have you tried baking the boards prior to assembly? We had this issue on a simple 4-layer board, and found t

Re: Baking a Populated PCB

Electronics Forum | Fri Jul 30 17:16:59 EDT 1999 | Dave F

| Hello Netters, | | I have a customer who wants us to aquaeos wash a PCB after all operations have been performed. The PWB is two layer FR4 with a Transformer, a Multichip Module with Conformal Coating, (6) 11" insulated wires that are tinned on e

Baking a Populated PCB

Electronics Forum | Fri Jul 30 14:53:01 EDT 1999 | Tom B.

Hello Netters, I have a customer who wants us to aquaeos wash a PCB after all operations have been performed. The PWB is two layer FR4 with a Transformer, a Multichip Module with Conformal Coating, (6) 11" insulated wires that are tinned on exposed

MSL Component - Popcorn Temp.

Electronics Forum | Wed Jul 04 09:58:50 EDT 2012 | daxman

Assuming that you have a saturated moisture-sensitive component: At what temperature would popcorning or internal component damage occur? I would guess that it would be at a temperature where water would boil, around 100 degrees? However, the JEDEC J


baking populated pcb searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830

High Throughput Reflow Oven

Training online, at your facility, or at one of our worldwide training centers"
Thermal Interface Material Dispensing

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
SMT feeders

Wave Soldering 101 Training Course