Full Site - : baking populated pcb (Page 32 of 86)

PWAs & PWB bake out requirements

Electronics Forum | Thu Aug 09 19:13:37 EDT 2007 | htran

DaveF, Our customer requirement is to comply with IPC-STD-001 but the J std doesn't specify the bake out temperature for populated boards and the moisture absortion rate. Right now we are baking the populated PWAs after aqueous wash at 80C at 18-48

PCBA rework

Electronics Forum | Tue Mar 09 12:13:27 EST 2004 | Gabriele

I want just to confirm what Dave suggested you. J-STD-033a, par 6. Boards Rework tells you plenty of useful informations. 6.1 Component removal, RWK and remount 6.1.1 Removal for Failure Analysi 6.1.2 Removal & Remount 6.2 Baking of Populated Boar

Re: Reflow Profile Dry Out Stage

Electronics Forum | Wed Dec 13 14:37:06 EST 2000 | Chris

I should explain that this bake out was performed after population. The solder paste slumped terribly after this bake out. However, after the back out and after reflow, no bridging.

Wash and bake of blank PCB's before assembly

Electronics Forum | Thu Jun 04 14:30:13 EDT 1998 | Igmar

I would appreciate any information concerning the wash and bake of blank Printed Circuit Boards before assembly. + Is it necessary to wash and bake PCB�s before assembly? + If any, what is the reason for wash and bake of PCB�s? + If any, what type of

Wash and bake of blank PCB's before assembly

Electronics Forum | Thu Feb 12 16:50:40 EST 1998 | Igmar

I would appreciate any information concerning the wash and bake of blank Printed Circuit Boards before assembly. + Is it necessary to wash and bake PCB�s before assembly? + If any, what is the reason for wash and bake of PCB�s? + If any, what type of

Re: moisture in pcb's how is it measured

Electronics Forum | Tue Oct 19 22:43:31 EDT 1999 | Stu Leech

We are deeply involved with this question because we have developed a much faster way to remove moisture from PCB's. PCB's absorb varying amounts of moisture at differing rates. The rate is influenced by the laminate type board configuration , loca

What is the MSL of a PCB

Electronics Forum | Wed Jan 14 12:40:46 EST 2015 | dyoungquist

MSL is used for components (and possibly bare pcbs) that are going to go through a reflow oven process in the future. In most cases, populated pcb assemblies will not be going through the reflow oven process again. Therefore, it is not necessary to

RoHS Board Delamination

Electronics Forum | Tue Oct 24 15:46:09 EDT 2006 | aj

Mark, The pcb manufacturer recommended we bake the boards , so we did. I even weighed a batch before and after and seen slight decrease possibly 0.1g in weight. However we still seen some delam after all this. I am confident our issue has nothing to

Board Baking recommendations

Electronics Forum | Mon Jan 08 10:41:50 EST 2007 | jaime39

If you bake the boards at 125 degrees celcius for about 4 hours it should work. I would also suggest that you talk to the PCB supplier to take care of this baking for you. NOTE: PCB�s with an Entek or any other type of OSP finish should not be baked.

PCB Baking

Electronics Forum | Wed Jul 12 21:40:22 EDT 2006 | YQ-Deng

How to bake the FR4 PCB?


baking populated pcb searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830