Full Site - : board / hasl thickness (Page 13 of 27)

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Tue May 26 15:27:36 EDT 1998 | Dave F

| | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and s

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Tue May 26 21:27:33 EDT 1998 | Earl Moon

| | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered a

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Wed May 27 11:19:34 EDT 1998 | Earl Moon

| | | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered

Stencil / Pad design

Electronics Forum | Mon Jun 28 10:17:44 EDT 2004 | davef

People like flat surfaces for placing and reflowing certain components, like fine pitch devices. Some board suppliers can supply HASL that is flat and well controlled from an amount of material stand-point. Unlike OSP, HASL has a wonderful shelf-li

Stencil / Pad design

Electronics Forum | Mon Jun 28 08:25:54 EDT 2004 | Scott Dodge

What is the difference between a smooth finish organic coated bare copper board for fine-pitch components and HASL finish?

board stretch and IPC -D-300G

Electronics Forum | Mon Nov 12 16:14:47 EST 2001 | davef

Yes!!! How can we assemble boards with 20 pitch when we allow 0.008� error to the master art? Excellent question!!! IPC-D-300G has nothing to do with assembler requirements. It is written by and for fabricators, so that they can be comfortable.

Dark Pad / Gold Embrittlement?

Electronics Forum | Wed Jul 26 10:06:19 EDT 2000 | Doug Philbrick

I have read many of the past threads on both topics and I still am not convinced I know the answer to the soldering problem we are encountering. I am hopping someone can help. I have a dense SMT board we are building and have been building for some

Re: DFM / DFT information

Electronics Forum | Thu Jul 13 22:20:38 EDT 2000 | Dave F

=10 mils larger than lead 3 silk screen legend text weight >=10 mils 4 pads >=15 mils larger than finished hole sizes 5 place through hole components on 50 mil grid 6 no silk screen legend text over vias (if vias not solder masked) or holes 7 so

Voiding in board to BGA joints

Electronics Forum | Tue Mar 09 07:51:12 EST 2004 | Bryan

Hello everyone: 1.I use Kester R244 63/37 solder paste. 2.Stencil thickness 6 mil. 3.Springdale Chipset. 4.PCB finish:HASL 5.Profile:Peak temp.:210~220C,time above 183C:60~90 seconds,time between 150~183C 60~90 seconds. 6.Reflow oven:Heller 1800 Voi

Lead Based Paste / Lead-Free BGA

Electronics Forum | Thu Nov 03 14:23:58 EST 2005 | Samir Nagheenanajar

Thank you for the advice. I am not so concerned with the "2nd reflow", as the same can be said for double sided reflowed PCBA's (the bottom-side parts essentially go through a 2nd reflow). As for the HASL, there is a formula in calculating how much


board / hasl thickness searches for Companies, Equipment, Machines, Suppliers & Information

Equipment Auction Automotive Electronics Supplier - Closure of Tier-One SMT Dvision: (10) ASM & Universal SMT Lines & Feeders Equipment as-new-as 2019! Dek | Koh Young | Speedline | Vitronics | Viscom

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
convection smt reflow ovens

World's Best Reflow Oven Customizable for Unique Applications
Electronic Solutions

High Precision Fluid Dispensers


Training online, at your facility, or at one of our worldwide training centers"