Full Site - : board / hasl thickness (Page 7 of 22)

HASL lead free thickness

Electronics Forum | Wed Nov 17 10:03:29 EST 2010 | scottp

Instead of a minimum thickness, we require no exposed copper or SnCu intermetallic. We've been having a lot of trouble lately with suppliers of SN100 HASL boards giving us pads with very irregular solder deposits with areas of exposed intermetallic.

Hasl thickness trends

Electronics Forum | Tue Sep 16 15:47:17 EDT 2003 | davef

First and most important, it doesn't matter dip who is down-wind of the rendering plant. The customer said, "I want bla bla bla." The supplier said, "I want to supply to the customer's order for bla bla bla and will deliver to that specification on

Re: Tin-Lead thickness on PWB's

Electronics Forum | Mon May 18 13:30:15 EDT 1998 | Earl Moon

| I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and solde

Re: Tin-Lead thickness on PWB's

Electronics Forum | Thu May 21 09:54:07 EDT 1998 | Justin Medernach

| I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and solde

Solder paste thickness measurement with laser machine

Electronics Forum | Thu Feb 23 13:56:21 EST 2006 | slthomas

I have dealt with it before and usually it's consistent, so you use some simple math to work around the issues. Now, if you have so much variability between different locations on your board for resist thickness, HASL thickness, etc., that it fouls

looking for HASL TIN thickness specification

Electronics Forum | Wed Sep 03 16:59:13 EDT 2008 | glennster

At a former employer we required HASL thicknes to be a minimum of 0.75 micron (30 microinches), as measured at the thinnest point on any given pad. This would generally assure a minimum 1 year solderability shelf life. Usually when we saw a soldera

looking for HASL TIN thickness specification

Electronics Forum | Tue Sep 02 13:26:52 EDT 2008 | vladig

You should have a few microns of Sn on a board. Vlad

looking for HASL TIN thickness specification

Electronics Forum | Wed Sep 03 19:54:23 EDT 2008 | vladig

Well, I'm not a sale person whatsoever. I'm a purely technical guy (even PhD :-)) who has been with the industry for quite a few years and I know very well what intermetallics means and how thck it should be for different board finishes and solders

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Tue May 26 14:50:07 EDT 1998 | Dave F

| | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and sol

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Tue May 26 20:18:09 EDT 1998 | Justin Medernach

| | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and


board / hasl thickness searches for Companies, Equipment, Machines, Suppliers & Information

IPC Training & Certification - Blackfox

High Resolution Fast Speed Industrial Cameras.
Sell Your Used SMT & Test Equipment

Component Placement 101 Training Course
SMT feeders

Reflow Soldering 101 Training Course
Online Equipment Auction Jabil Monterrey MX Aug 19, 2024

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
design with ease with Win Source obselete parts and supplies

Private label coffee for your company - your logo & message on each bag!