Full Site - : candle wax coated electronics (Page 3 of 4)

Nano ProTek Coating

Electronics Forum | Thu Jul 21 11:13:25 EDT 2011 | kahrpr

we use turtle wax on a more serous note, I bet those two products are similar in the fact it you fill the ridges in the aperture walls you will get better release. They may be closer than you think.

SMT Environment

Electronics Forum | Thu Aug 10 10:13:11 EDT 2006 | pjc

I have never seen any industry standards for setting up an SMT assembly facility, but I�ll offer some basic advise. An ideal SMT assembly facility is one that is clean and well lit and has environmental controls to maintain temp and RH. Temp of 24C (

AR/UR Coating Application

Electronics Forum | Thu Feb 01 07:41:01 EST 2018 | dontfeedphils

Interesting, never heard of using wax as a coating mask. Not sure how well the AR coating would hold up to a hot alkaline wash (unless you have experience with it), but that stuff usually starts to flake off/de-wet if you just look at it wrong. I'm

Solder balls on pads - lead free

Electronics Forum | Wed Sep 19 10:38:58 EDT 2012 | mark25y2001

It's both solderpaste or PCB pad problem... 1st it's possible that your PCB exposure problem or old stocks, remedy? try to bake your PWB. 2nd, it's possible that PWB coating (wax) are more ticked so that solder paste flux are cannot penetrate to clea

Paste printing fine pitch components

Electronics Forum | Thu Oct 17 21:13:35 EDT 2013 | hegemon

But where does it go, that it needs to be refreshed or replenished on the stencil? Does that "just like wax" product wind up in my solder joints, no matter how small the percentage, and would it then qualify as a contaminant? I heard there are some (

Smurf Coats

Electronics Forum | Tue Dec 11 20:22:33 EST 2001 | mparker

in your example, wool clothing and prairie winter ionization makes sense. Smocks would be an improvement to contain the potential of static build up. If you go to dress codes, then you run the risk of having to provide uniforms or pay a laundry allow

Adhesion of conformal coating to plastic components

Electronics Forum | Tue Jun 02 14:32:58 EDT 1998 | Chris Fontaine

We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not alwa

Re: Adhesion of conformal coating to plastic components

Electronics Forum | Tue Jun 02 15:53:32 EDT 1998 | Earl Moon

| We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not al

Re: Adhesion of conformal coating to plastic components

Electronics Forum | Wed Jun 03 07:13:27 EDT 1998 | Tom Tellinghuisen

| We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not al

Re: Adhesion of conformal coating to plastic components

Electronics Forum | Tue Jun 02 17:36:43 EDT 1998 | Chris Fontaine

| | We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not


candle wax coated electronics searches for Companies, Equipment, Machines, Suppliers & Information

Nordson Electronics Solutions
Nordson Electronics Solutions

Nordson Electronics Solutions makes reliable electronics an everyday reality. Our ASYMTEK, MARCH, and SELECT brands deliver precision fluid dispensing, conformal coating, plasma treatment and selective soldering equipment.

Manufacturer

2747 Loker Ave West
Carlsbad, CA USA

Phone: 18002796835