Full Site - : coating on tall part (Page 6 of 7)

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Thu May 28 05:43:33 EDT 1998 | Earl Moon

| Hey yooze guys! | Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) | Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any p

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Wed May 27 21:05:30 EDT 1998 | Steve Gregory

Hey yooze guys! Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any posts f

MYDATA - how to forse parts on Hydra head

Electronics Forum | Mon Dec 19 07:55:30 EST 2016 | bk

I am assuming that these are the round aluminum electrolytic caps. The problem may be that they are too wide to put on 2 hydra heads next to each other. Plus the hydra heads are not that great at placing tall parts. I would not let the hydra place th

Local Cleaning Post Rework on PCB with Conformal Coating

Electronics Forum | Mon Apr 02 10:11:58 EDT 2012 | jdumont

Wondering how you guys do this. Scenario: You have to rework a part (small IC or resistor) on a board that has already been conformal coated with acrylic. What do you do with the post soldering residues before you cover it up with fresh coating?

Re: Need suggestions on conformal coat curing oven

Electronics Forum | Wed Apr 14 17:13:08 EDT 1999 | Stephen Oltmann

| I need to cure conformal coat on a 19" x 15" board. The material needs 7 - 10 minutes at 100deg C, but I have limited floorspace so I'm looking for an oven with about 36 inches heated length and 18 or more inch wide belt. The material we are consid

Re: Need suggestions on conformal coat curing oven

Electronics Forum | Wed Apr 14 17:14:49 EDT 1999 | Stephen Oltmann

Check with BTU. They have dryers in the length you need. Good luck! | | I need to cure conformal coat on a 19" x 15" board. The material needs 7 - 10 minutes at 100deg C, but I have limited floorspace so I'm looking for an oven with about 36 inches

Re: Need suggestions on conformal coat curing oven

Electronics Forum | Sat Apr 17 11:56:04 EDT 1999 | Graham Naisbitt

Mike First, you MUST make sure the oven used is extracted. The coating will contain TDI. This is not nice. You would be better considering a silicone solventless. Try contacting HumiSeal. They had a material on the TAC line at Nepcon West that lo


coating on tall part searches for Companies, Equipment, Machines, Suppliers & Information

Count On Tools, Inc.
Count On Tools, Inc.

COT specializes in high quality SMT nozzles and consumables for pick and place machines. We provide special engineering design service of custom nozzles for those unique and odd components.

Manufacturer

2481 Hilton Drive
Gainesville, GA USA

Phone: (770) 538-0411

Electronics Equipment Consignment

High Precision Fluid Dispensers


Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
SMT feeders

World's Best Reflow Oven Customizable for Unique Applications
SMT feeders

We offer SMT Nozzles, feeders and spare parts globally. Find out more
design with ease with Win Source obselete parts and supplies

Internet marketing services for manufacturing companies