Electronics Forum | Tue May 26 21:27:33 EDT 1998 | Earl Moon
| | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered a
Electronics Forum | Wed May 27 11:19:34 EDT 1998 | Earl Moon
| | | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered
Electronics Forum | Tue May 26 15:27:36 EDT 1998 | Dave F
| | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and s
Electronics Forum | Tue May 26 14:50:07 EDT 1998 | Dave F
| | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and sol
Electronics Forum | Thu May 28 07:25:58 EDT 1998 | Earl Moon
| Hey yooze guys! | Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) | Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any p
Electronics Forum | Thu May 28 05:43:33 EDT 1998 | Earl Moon
| Hey yooze guys! | Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) | Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any p
Electronics Forum | Wed May 27 21:05:30 EDT 1998 | Steve Gregory
Hey yooze guys! Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any posts f
Electronics Forum | Mon Dec 19 07:55:30 EST 2016 | bk
I am assuming that these are the round aluminum electrolytic caps. The problem may be that they are too wide to put on 2 hydra heads next to each other. Plus the hydra heads are not that great at placing tall parts. I would not let the hydra place th
COT specializes in high quality SMT nozzles and consumables for pick and place machines. We provide special engineering design service of custom nozzles for those unique and odd components.
2481 Hilton Drive
Gainesville, GA USA
Phone: (770) 538-0411