Conformal Coat Thickness

Electronics Forum | Mon Jul 23 16:17:19 EDT 2007 | mleber

We have not had the best of luck with wet film. I agree on your statement. Depending on the mix and amount of solvent your results will vary. We were looking for something easy, accurate and foolproof.

Bubbles in Conformal Coating

Electronics Forum | Tue Feb 03 13:47:59 EST 2009 | grics

I would also suggest looking at your ramp rate in the cure oven. We noticed that accelerated heating increased the "gas out" of the solvent. We run 1A33 and and do not exceed a .5/degC ramp rate.

Info on OSP PCB�s

Electronics Forum | Tue Jun 05 21:14:10 EDT 2001 | davef

You aren't going to post our stuff on your "Hey, I'm the wizard site", are you? Board fab, Pad coatings, OSP 1 OSPs: Imidazole (Via Systems) is good. Entek (Enthone) works, but requires strict thickness control in fab. 2 Enthone CU56 allows one t

Cleaning for conformal coat

Electronics Forum | Fri Jan 25 12:14:18 EST 2013 | johng

I'm using urethane conformal coat and have fisheyes and dewetting after coating even though the PWAs have been through the wash cycle twice. I'm looking at using Ionox 13302 in an ultrasonic cleaner as a short term solution until root cause can be id

Cleaning for conformal coat

Electronics Forum | Fri Jan 25 12:15:04 EST 2013 | johng

I'm using urethane conformal coat and have fisheyes and dewetting after coating even though the PWAs have been through the wash cycle twice. I'm looking at using Ionox 13302 in an ultrasonic cleaner as a short term solution until root cause can be id

Conformal Coat peeling

Electronics Forum | Tue Apr 14 17:39:34 EDT 2009 | gregoryyork

Sorry been away for a while. It is actually due to high boiling solvents or plasticizers leaching from the porous resist that kills the cure as it puddles out and has nothing to adhere to. We do have some wipes to check the cure and are looking to ma

Re: Conformal Coating that doesn't require fancy equipment...

Electronics Forum | Sat Jul 25 11:11:09 EDT 1998 | Mike Moninger

| Be consistant on: | 1 Keeping the coating material thinned. | 2 Using the same dipping motion on each board. Amen on thinning the coating, and you might also be concerned about the curing mechanism for the coating. Moisture-cured and 2 component

Re: measuring board/assy cleanliness

Electronics Forum | Wed Oct 18 16:33:26 EDT 2000 | Dave F

Mike: An omega meter has very little to do with ion chromatography. * IPC TM-650, 2.3.25B, Detection and Measurement of Ionizable Surface Contaminants is a process control method that washes boards with an isopropanol / water solution and measures

how clean is clean?

Electronics Forum | Thu May 26 19:32:13 EDT 2005 | Mike Konrad

Three popular methods: Resistivity of Solvent Extract (ROSE) Test Method IPC-TM-650 2.3.25: The ROSE test method is used as a process control tool to detect the presence of bulk ionics. The IPC upper limit is set at 10.0 *g/NaCl/in2. This test is p

Conformal coat material dispensed through epoxy needle?

Electronics Forum | Tue Feb 07 10:25:37 EST 2017 | ttheis

Thanks for the tip. I'm still getting familiar with the machine by reading the manuals as I have time. Was wondering what type of solvent you use to clean the dispensing mechanism parts? Or do you not clean anything and simply dispose of the syring p


coating solvent searches for Companies, Equipment, Machines, Suppliers & Information

Electronics Equipment Consignment

High Throughput Reflow Oven
PCB Handling with CE

High Precision Fluid Dispensers
Fluid Dispensing, Staking, TIM, Solder Paste

World's Best Reflow Oven Customizable for Unique Applications
Selective soldering solutions with Jade soldering machine

High Resolution Fast Speed Industrial Cameras.