80/20 Au/Sn Solder and Proper FLux Selection

Electronics Forum | Mon Jan 17 17:38:29 EST 2011 | bandjwet

All: I am reaching out to get some suggestions on the right flux to use as well as a recommended cleaning process for soldering a KOVAR RF shield using 80/20 Au/Sn solder to a ceramic hybrid. The recommended profile is 4-5 min at 280C and at least

lid soldering problems (CQFP, Au/Sn solder)

Electronics Forum | Thu Sep 17 07:06:15 EDT 1998 | joakim fagerlund

We have problems with voids when we solder lids to ceramic flatpackages. The sealring of the package is gold(100 micro inches or 2.5 micro meters)with a underlayer of Nickel The solder is attached to the lid (preform) and the solder material is Au/S

Express Newsletter: coining 80/20 au/sn (8)

Partner Websites: coining 80/20 au/sn (3)

US0683966

GPD Global | https://www.gpd-global.com/co_website/pdf/GPD-Global-CMRT-2021.xlsx

.” as a tin refinery 19. Updated “ATI Metalworking Products” to its proper full name “ATI Tungsten Materials” 20. Updated “China Minmetals Corp

GPD Global


coining 80/20 au/sn searches for Companies, Equipment, Machines, Suppliers & Information

Sm t t net
  1 2 Next
Encapsulation Dispensing, Dam and Fill, Glob Top, CSOB

We offer SMT Nozzles, feeders and spare parts globally. Find out more
SMT feeders

High Precision Fluid Dispensers
SMT feeders

Wave Soldering 101 Training Course
Circuit Board, PCB Assembly & electronics manufacturing service provider

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.