Full Site - : copper leaching (Page 2 of 6)

Re: Surface Mount assemblies IPC Standards

Electronics Forum | Thu Aug 26 10:03:17 EDT 1999 | Sal

| | Could somebody tell me what means Leaching, ie: "Leaching of terminal end face exposing the ceramic"? | | | Roberto: Leaching, according to the SMTnet Library of Terms: | | Leaching. Dissolution of a metal coating into liquid solder. Nickel ba

Re: Surface Mount assemblies IPC Standards

Electronics Forum | Tue Jun 29 18:35:59 EDT 1999 | JohnW

| | Could somebody tell me what means Leaching, ie: "Leaching of terminal end face exposing the ceramic"? | | | Roberto: Leaching, according to the SMTnet Library of Terms: | | Leaching. Dissolution of a metal coating into liquid solder. Nickel ba

solder balls on pcb

Electronics Forum | Tue Nov 04 12:58:17 EST 2008 | smt123

I have to agree with Patrick here. This image appears to show a board that is NOT HASL as there is what appears to be a copper pad in the upper portion of the image. But then again the arrow tip appears to be white and I woudl expect that to be red s

Re: Surface Mount assemblies IPC Standards

Electronics Forum | Thu Jul 01 16:43:52 EDT 1999 | Dave F

| | | Could somebody tell me what means Leaching, ie: "Leaching of terminal end face exposing the ceramic"? | | | | | Roberto: Leaching, according to the SMTnet Library of Terms: | | | | Leaching. Dissolution of a metal coating into liquid solder.

Re: Surface Mount assemblies IPC Standards

Electronics Forum | Wed Jun 30 11:09:24 EDT 1999 | John Thorup

| | | Could somebody tell me what means Leaching, ie: "Leaching of terminal end face exposing the ceramic"? | | | | | Roberto: Leaching, according to the SMTnet Library of Terms: | | | | Leaching. Dissolution of a metal coating into liquid solder.

can silver plating be used as barrier when soldering brass to copper? silver plate the brass?

Electronics Forum | Thu Jun 08 07:56:34 EDT 2017 | jkitt84

In an excellent previous thread davef mentions brass should be plated prior to soldering to prevent zinc leaching from the brass. It is reported once the zinc leaches, the joint is weak. He recommends copper or nickel plating. Would silver plating w

Re: Surface Mount assemblies IPC Standards

Electronics Forum | Thu Jul 01 16:57:14 EDT 1999 | JohnW

| | | | Could somebody tell me what means Leaching, ie: "Leaching of terminal end face exposing the ceramic"? | | | | | | | Roberto: Leaching, according to the SMTnet Library of Terms: | | | | | | Leaching. Dissolution of a metal coating into liqu

Re: Surface Mount assemblies IPC Standards

Electronics Forum | Thu Jul 01 20:56:57 EDT 1999 | Dave F

| | | | | Could somebody tell me what means Leaching, ie: "Leaching of terminal end face exposing the ceramic"? | | | | | | | | | Roberto: Leaching, according to the SMTnet Library of Terms: | | | | | | | | Leaching. Dissolution of a metal coating

Re: Black spots on gold finish pads.

Electronics Forum | Tue Dec 01 07:24:44 EST 1998 | Earl Moon

| Hi folks , | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our inspection

Re: Black spots on gold finish pads.

Electronics Forum | Tue Dec 01 07:54:49 EST 1998 | kallol chakraborty

| | Hi folks , | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our inspec


copper leaching searches for Companies, Equipment, Machines, Suppliers & Information

SMT feeders

Best Reflow Oven
Selective soldering solutions with Jade soldering machine

High Precision Fluid Dispensers
Selective soldering solutions with Jade soldering machine

High Throughput Reflow Oven
SMTAI 2024 - SMTA International

World's Best Reflow Oven Customizable for Unique Applications