Electronics Forum | Mon May 18 20:57:06 EDT 1998 | Earl Moon
.025" pitch so the only problem we run into is too much HASL on the adhesive side causing improper glue dispense. | As Earl keeps saying HASL thickness is hard to impossible to control. I think we need to look hard at OSP's again but then you get in
Electronics Forum | Mon May 18 22:54:04 EDT 1998 | Dave F
.025" pitch so the only problem we run into is too much HASL on the adhesive side causing improper glue dispense. | | As Earl keeps saying HASL thickness is hard to impossible to control. I think we need to look hard at OSP's again but then you get
Electronics Forum | Mon May 18 13:30:15 EDT 1998 | Earl Moon
| I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and solde
Electronics Forum | Fri May 01 08:15:36 EDT 2009 | davef
Scavenging Methods [Improve Solder Scavenging of Large Area-array Sites, SMT, Laurence Harvilchuck, process research engineer, Unovis Solutions, harvilch@unovis-solutions.com] Two common methods exist for scavenging residual solder on the site for s
Electronics Forum | Mon Aug 28 15:34:19 EDT 2000 | Steve Harshbarger
Hello Ramon, This is a very common problem that usually can be overcome. Can you tell me the flux type you are using (manufacturer, and flux number)? Has your board vendor, or type of PCB's changed (are they entec coated - bare copper)? What is t
Electronics Forum | Tue Aug 31 12:42:45 EDT 1999 | Charles Barker
****************************************** ***************** HELP! *************** ****************************************** We are having a special ceramic smt board made. The boards are 16-up arrays that have smt pads on both sides. Only thre
Electronics Forum | Fri May 28 07:37:52 EDT 1999 | Steve Cheung
Yes l know this problem keeps cropping up on the forum but l've missed some of the follow-ups. Our problem is that the lifting only occurs on 3% of production so actually detecting an improvement is difficult. We're actually having to inspect 144 p
Electronics Forum | Thu Dec 08 01:05:34 EST 2005 | Mike_Kennedy
Our new PCB supplier can give us a 20% price reduction if we convert from an ENIG finish to a FLASH gold finish. My uderstanding between the two is as follows: ENIG - Nickel is plated over copper and then immersed in Gold which forms a self limited f
Electronics Forum | Wed Dec 14 07:34:33 EST 2005 | davef
Mike Ozzy If I came to your house, I wouldn't punch you. I'd make you buy me beer. Vern Solberg; Tessera Technologies Inc., 3099 Orchard Dr, San Jose, CA 95134; 408 568 3734 F408 894 0768 vsolberg at tessera dot com. If that doesn't work try: Tes
Electronics Forum | Thu Dec 14 10:14:04 EST 2000 | PeteB
Jacqueline, Asuming you mean immersion silver: Advantages - Very flat finish compared to HASL, more easily solderable than bare copper with OSP and more process tolerant than this in our experience, reasonable shelf life, cheaper than immersion gol