Electronics Forum | Wed Jul 11 14:45:22 EDT 2007 | samir
ECD, KIC, or any mfgr. of thermal profiling devices will charge a premium for "simple stuff". For example, ECD charges a grand for their "flux-o-meter", which is just a PCB with a hole pattern, a pallet, and pH-sensitive paper. You can easily ma
Electronics Forum | Tue Sep 18 07:52:29 EDT 2007 | davef
Does the change from supplier to supplier as a result of: * Board definition? * Differences in processing at fabs? 3 Specification Fir Tree General Technical Specification 3a Design/Layout: * IPC-2221 * IPC-2222 3b PCB Fab: * IPC-6011 * IPC-6012 * I
Electronics Forum | Thu May 01 12:46:19 EDT 2008 | dphilbrick
Thanks for the link Samir. Although this thread does have some good info in it I don't think it is hitting the exact point I am trying to resolve. This seems to talk to a one profile fits all for running lead and lead free paste. I want to know about
Electronics Forum | Tue Nov 05 09:57:45 EST 2013 | cuperpeter
Hello All, We have a problem with dewetting of solder paste. Problem is most visible on the pads without components (see attached pictures) and occurs randomly, 20% of PCB's. Pcb supplier sent us a cross-section of pads with thickness of Cu, Ni and
Electronics Forum | Tue May 02 17:11:17 EDT 2000 | John
My company just purchased a Vecta (E-vert) wave soldering machine. Bridging has become a serious issue, both on SMT components and thru hole. We are currently seeing about 500 ppm. The products that are being run now were run previously on our old
Electronics Forum | Mon Mar 20 15:48:52 EST 2000 | Shane Lay
We are planning on converting to a no-clean soldering chemistry and will need to replace our water soluble liquid solder mask as a result. Does anyone know of a dispensable, "peelable" solder mask I can evaluate? It would be nice to find one that i
Electronics Forum | Thu Jul 20 16:45:54 EDT 2000 | Darby
Good morning Bob. Darby from Australia here. We sometimes see an orange peel type finish on our reflow solder joints when viewed under the microscope. Any ideas on what causes this ? Should I worry about it. I use a straight rise profile ( no "platea
Electronics Forum | Tue Jun 19 12:15:45 EDT 2001 | Gil Zweig
I have made reference to X-ray Ball Bond Signatures a number of times, and I cannot overstate the importance of quickly qualifying the overall ball bond pattern as either uniform in size and shape or not. Software is available that will make this qua
Electronics Forum | Mon Jun 18 19:32:58 EDT 2001 | Gil Zweig
I believe that at the present time the industry really does not know how to use x-ray inspection apart from indentifying the obvious defects such as shorts, missing balls and gross solder voids. The real utility of x-ray inspection is to recognize: 1
Electronics Forum | Tue Jun 26 09:37:28 EDT 2001 | Steve Vargas
We are interested in doing some further studies on our cleaning process, particularly with respect to how well we can clean underneath low profile components. As an SMT subcontractor, we'd ideally like to qualify our chemistry/cleaning process to cer