BGA attach eval.

Electronics Forum | Tue Apr 01 09:58:52 EST 2003 | davef

You're entirely correct. The gold is most likely gone away. [Don't forget you can check if the surface is still solderable with a hand soldering iron.] We're not sure it it will give you the results you seek, but consider using a dye penetrant fai

Dye and Pry

Electronics Forum | Wed Mar 12 07:33:40 EDT 2008 | callckq

Hi All, One PCBA failed test after went through the Shock Test(Vibration) and suspected to be BGA solder ball crack. We performed dye and pry and found PCB's pad lifted with red mark ink penetrate pad underneath, what does this mean? Can I say the

Re: Suspect BGAs

Electronics Forum | Wed Mar 17 17:14:49 EST 1999 | Michael Allen

Another test to consider is dye penetrant analysis. The technique involves flooding the area beneath the soldered part with dye (preferably a bright color, like red). After drying the board+dye in an oven, you peel or torque the part off and inspec

Sm t t t t t t net
Previous 2 3 4 5 6 7  

dye penetration to solder searches for Companies, Equipment, Machines, Suppliers & Information

Best SMT Reflow Oven

High Throughput Reflow Oven
Fluid Dispensing, Staking, TIM, Solder Paste

Training online, at your facility, or at one of our worldwide training centers"
PCB Handling with CE

World's Best Reflow Oven Customizable for Unique Applications
SMTAI 2024 - SMTA International

Wave Soldering 101 Training Course
PCB separator

Training online, at your facility, or at one of our worldwide training centers"