I have experience in this. My company offers Lead free SMT and Wave soldering. I have processed ImSn, ImAg, Enig, OSP in both smt and wave. Yes, silver leaching will occur. Yes, copper leaching will occur. High tin content solders disolve everyt
Electronics Forum | Fri May 07 00:52:24 EDT 2010 | boardhouse
Hi Derek, just curious of one thing - are the vias within the BGA's the only vias covered or are all vias on the board covered. Just trying to figure out what is making this area different from the rest of the board. Regarding leaching, I do not be