Electronics Forum | Thu Mar 24 15:29:46 EST 2005 | Claude_Couture
other than the fact that silver is a better conductor of heat, I can't think of anything.
Electronics Forum | Mon Jul 05 03:44:53 EDT 2004 | johnwnz
Dave, I'm going to disagree with you on the ENIG, it's my 3rd choice only just beating out OSP for that 4th spot. 1. Immersion Silver - cheaper than ENIG, as flat and no issues with Brittle interface (black pad) or Gold Embrittlement) Longer shelf l
Electronics Forum | Thu Jul 28 09:47:06 EDT 2005 | fctassembly
Hello Carl, The main reason there is little information on lead free soldering to ENIG is because most of the lead free soldering to date has been Japanese consumer products. To keep costs down, the major surface coating used has been OSP copper. It
Electronics Forum | Mon Jan 29 12:09:55 EST 2018 | fluxgate
I am working on a magnetic sensors design and noticed that my measured magnetic field bias shifts over time. I have studied the bare PCB and measured that it can be magnetized with a strong magnet. I tested two blank (unpopulated PCBS). The first PC
Electronics Forum | Tue Jun 06 19:03:59 EDT 2017 | zsoden
Hi Steve, I just confirmed with the manufacturer and the HASL is tin/lead (or it is supposed to be, at least). Any suggestions for how to test for nickel vs tin/lead? We're using an alcohol based no-clean flux from Alpha.
Electronics Forum | Wed Nov 21 05:57:30 EST 2018 | premkumar_haribabu
Hi Robl, Thanks for your qucik reply!! , i understand if we use aggresive flux that we can impove solder wetting over nickel plate vs PCB pads & we need to solder through 12 zones reflow oven. Prem
Electronics Forum | Thu Feb 22 20:34:25 EST 2007 | davef
This [ http://www.smtnet.com/library/index.cfm?fuseaction=view_article_html&file=no_hasl ] describes HASL [hot air solder leveling], as well as other common types of solderability protection. It goes on the discuss the impact of the use of these coa
Electronics Forum | Tue Jan 31 14:35:55 EST 2012 | hegemon
1. (NCMR) Non Conforming material report to your customer if you have signed up for a lead free job. Send everything back and tell him to replace the entire lot with correct material. or 2. Request a Change order from your customer, changing the
Electronics Forum | Wed May 14 12:42:16 EDT 2008 | rgduval
Dave, Realized I didn't respond to one of your questions. We pasted and reflowed one board, with no components. This board exhibited extreme dewetting on all pads. The board was LF-HASL, and the paste was Qualitek (which we've used for approximat
Electronics Forum | Wed Jun 10 18:28:57 EDT 1998 | Al
| Okay, here's a stupid question. What exactly is HASL and OSP? We are going to delve into this technology where I work and I want to utilize the wealth of knowledge here to make life easier. Specifically, what are the differences, the advantages, di