Electronics Forum | Tue Jan 12 15:29:40 EST 2010 | davef
What is your concern regarding voiding in QFN solder connections?
Electronics Forum | Thu Mar 17 03:07:17 EST 2005 | Chua
Hi, We are running lead free at wave solder now and the spray flux system is down. If we are going to able the flux manually, what problem will we be facing with the excess flux able. Appreciate for the advise.
Electronics Forum | Fri Dec 03 15:56:47 EST 2004 | Indy
Hi Everyone, Could someone please tell me - What happens if a N-type connector having chromate coating over silver plating is hand soldering to a PCB. Does the Chromate coating form a compound with silver, Or does it come off while cleaning excess
Electronics Forum | Tue Jan 16 20:44:07 EST 2007 | davef
Bridging Causes: Insufficient flux, Excessive pre-heat, High conveyor speed, Solder contamination Look here: * http://www.smtnet.com/library/files/upload/Reflow%20Wave%20Poster.pdf * http://smt.pennnet.com/Articles/Article_Display.cfm?Section=Archi
Electronics Forum | Sat Jun 05 13:38:22 EDT 2021 | ppcbs
For Linear Tech LGA's we solder bump the LGA using a .30mm solder ball then reflow with a tacky flux. This will provide a void free solder joint and adds a little height to the solder joint in case you use a flux that you want to clean from under th
Electronics Forum | Mon Sep 21 20:45:55 EDT 2009 | davef
10.4. Pre-Cure Examination. Immediately after material application, the uncured conformal coating shall be examined for: a. Bubbles and Air Entrapments. These defects shall be broken by vacuum, with a sharp probe, or other appropriate tools. b. Bridg
Electronics Forum | Tue Dec 01 07:24:44 EST 1998 | Earl Moon
| Hi folks , | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our inspection
Electronics Forum | Tue Dec 01 07:54:49 EST 1998 | kallol chakraborty
| | Hi folks , | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our inspec
Electronics Forum | Fri May 21 15:20:26 EDT 1999 | JohnW
| I normally handle the soldering issues for this facility but a question was asked of me -- What the H@## is this stuff and what is causing it? Was wondering of I could get some input from any Guru on plating issues. Need info ASAP!!!!!!!!!!!!!!!!!
COT specializes in high quality SMT nozzles and consumables for pick and place machines. We provide special engineering design service of custom nozzles for those unique and odd components.