Re: Help me increase my first pass yields

Electronics Forum | Fri Jun 05 13:06:14 EDT 1998 | Steve Schrader

| If you could measure and chart 3 variables in my process, what would they be? | The boards that I produce are on panels that are 12up and 2x4 up. All boards are single sided paper base w/o plated thru holes. They are on scored panels that measure

Re: Help me increase my first pass yields

Electronics Forum | Thu Jun 04 15:41:07 EDT 1998 | Chrys

| If you could measure and chart 3 variables in my process, what would they be? | The boards that I produce are on panels that are 12up and 2x4 up. All boards are single sided paper base w/o plated thru holes. They are on scored panels that measure

Re: Cleaning No Clean Wave Solder Carriers

Electronics Forum | Fri Jan 08 10:07:26 EST 1999 | Chrys

| I'm in the process of moving from water washable flux to a full no clean process for the wave soldering process, thing's seem to be going well (so far...). | The one problem I still have is cleaning the wave solder carrier's to remove the no clean

Re: Cleaning No Clean Wave Solder Carriers

Electronics Forum | Mon Jan 18 19:53:58 EST 1999 | Rob F

| | I'm in the process of moving from water washable flux to a full no clean process for the wave soldering process, thing's seem to be going well (so far...). | | The one problem I still have is cleaning the wave solder carrier's to remove the no cl

changing from no-clean to clean

Electronics Forum | Tue May 21 17:16:51 EDT 2002 | davef

Larry, Yes, no matter how much you�d like to avoid using NC, you probably will have to start using the stuff, if the design [sales, in your case] types have their way. We can clean WS under 1mm and 1.25mm pitch BGA. For 0.8mm pitch BGA, we use NC.

Quad IVc Part rejection issue

Electronics Forum | Sun Sep 09 02:24:04 EDT 2012 | audere

More lube on the O-Rings caused lots of problems. Nozzles would drop downward at times. So I pulled everything out and started from scratch. Testing 3 new Z-Rods, 4 used Z-Rods in good shape (replaced the O-Rings) and around 20 nozzles - the proces

Re: Proflow of DEK screen printer

Electronics Forum | Wed Sep 08 08:25:26 EDT 1999 | Brad Kendall

Listed below are the issues Viking has been experiencing since the | installation of the Proflow Head: | 1. After installing new 350mm Wiper foil with metal | strip glued on it, It worked for about a week and suddenly meta

Rep Responses in Forum, Possible Guidelines

Electronics Forum | Mon Oct 14 12:56:50 EDT 2002 | davef

His technical contribution to the forum. From these 24 postings, we can see that 75% of Sean�s postings have a decided commercial bent, as followings: * Could be argued that the posting is a good technical response. Percent of postings 25%. * Could

Juki KE-750 T & Z servo failures

Electronics Forum | Fri Aug 30 15:44:51 EDT 2019 | valentink

I will try outline Theta and Z-axis servo issues, we were facing last time. Story behind. Our 750 is used seldom and last time after switching it on initialization procedure ends with T axis of right head: Servo alarm. Opening front cover of 750 two

Process Engineering/Maintenance Technician

Career Center | Fredericksburg, Virginia USA | Engineering,Maintenance,Management,Production,Quality Control

• Certified CP643 Loader Calibration – FUJI American Chicago, IL 2001. • Certified - Cookson Performance Solutions BTU - PARAGON - P150 Oven – Maintenance & Electrical Troubleshooting Charlotte, NC 2001. • Certified UNIVERSAL (GSM) Platform: Operat


glue removing searches for Companies, Equipment, Machines, Suppliers & Information

Selective soldering solutions with Jade soldering machine

Stencil Printing 101 Training Course
Selective soldering solutions with Jade soldering machine

High Precision Fluid Dispensers
SMTAI 2024 - SMTA International

World's Best Reflow Oven Customizable for Unique Applications