Electronics Forum | Fri Dec 16 08:00:26 EST 2005 | jax
What you are most likely dealing with: Insufficient Pure Sn layer ( multiple causes ) Because elevated temperatures accelerate the diffusion process, the thickness of the Pure Sn layer will reduce during every thermal cycle... ( bakeing PCBs, S
Electronics Forum | Wed Jul 02 12:42:58 EDT 2003 | slthomas
Not sure how else to describe this. We've received some boards (1/2" x 3.5" x .0325" board built on panels of 24) with numerous resistors showing separation of the solder from the metallization at the top of the joint. There are 26 0805's on the bo
Electronics Forum | Fri Dec 14 13:58:07 EST 2001 | slthomas
This is one I haven't seen before (not in this context, anyway). We have an assembly that we have the SMT done out of house on, because of the high volumes. The boards have two distinct characteristics with respect to the appearance of the solder jo
Electronics Forum | Tue May 31 11:56:12 EDT 2005 | chunks
Hi Matt, Get definitive answers! Contamination on the HASL finish?: From the pix you posted, it looks like something fishy is going on. I�d reject them back to the board house and demand an answer. Most board houses and purchasing people will g
Electronics Forum | Fri Jun 04 15:04:16 EDT 1999 | Earl Moon
| I'm encountering a new problem at my new company that I haven't encountered before in my past life - and that's Wave Soldering VIA holes. | | We've been getting a rash of defects that we call in this company, "insufficient solder in VIA hole." The
Electronics Forum | Mon May 14 17:14:07 EDT 2001 | davef
First, consider checking the fine SMTnet Archives. Look for threads on "white tin", in addition to "immersion tin". We�ve had a cuppla good ones of late. Merix [http://www.merix.com] gives a good comparison of different solderability preservatives
Electronics Forum | Wed Jul 25 23:35:18 EDT 2001 | mugen
my guys SOP : Round #1 1) take double-side tape, and peel it flat to the PCB. 2) process this PCB only through P&P SMT. 3) confirm the SMD placement Round #2 4) take thin plastic sheet and tape corners flat to the PCB. 5) solder paste print over t
Electronics Forum | Wed Jul 25 23:37:11 EDT 2001 | mugen
my guys SOP : Round #1 1) take double-side tape, and peel it flat to the PCB. 2) process this PCB only through P&P SMT. 3) confirm the SMD placement Round #2 4) take thin plastic sheet and tape corners flat to the PCB. 5) solder paste print over t
Electronics Forum | Wed Sep 29 23:54:07 EDT 1999 | Dreamsniper
Hi everyone, Greetings! I�ve got a 2-layered through-hole PCB�s having the following problems: Solder Mask peels after wave soldering at random locations and only at the bootom side of the PCB Insufficient Solder and some solder never make it to t
Electronics Forum | Thu Jun 03 20:09:56 EDT 1999 | C.K.
I'm encountering a new problem at my new company that I haven't encountered before in my past life - and that's Wave Soldering VIA holes. We've been getting a rash of defects that we call in this company, "insufficient solder in VIA hole." These def