Electronics Forum | Wed Jun 01 01:08:43 EDT 2011 | boardhouse

Hi Aj, for the most part we have gotten away from calling out specific material and instead calling out IPC4101 back slashes to needed requirements. But if you are just looking for what most domestic shops have switch to you would be looking at 370

Why delamination happens on PCBs?

Electronics Forum | Wed Jun 22 02:30:33 EDT 2011 | boardhouse

if its a RoHs Assembly they should be using an FR4 material designed with higher TD to handle higher Assembly temps. 370HR,IT158, IT180, 4000-29 just to name a few that would be suitable. Standard FR4 material is not designed to handle the higher as