Re: Time to use alternative finishing ???

Electronics Forum | Mon Sep 13 06:23:06 EDT 1999 | Earl Moon

| | We have a product, with various PWBs, with over 600 parts each one (We are a low Volume/high mix company with an average component placement per PCB between 250 to 300 parts). This PWBs have 7 to 10, 20 mils pitch parts. We are having problems wi

Re: Time to use alternative finishing ???

Electronics Forum | Mon Sep 13 05:02:19 EDT 1999 | Brian

| We have a product, with various PWBs, with over 600 parts each one (We are a low Volume/high mix company with an average component placement per PCB between 250 to 300 parts). This PWBs have 7 to 10, 20 mils pitch parts. We are having problems with

Nonwetting Components - why won't components wet to solder?

Electronics Forum | Thu Jan 25 16:58:53 EST 2007 | wagoner

We are using tin-lead solder. The components could be lead free components, they probably are. I will check the plating on the components and investigate changing it.

Nonwetting Components - why won't components wet to solder?

Electronics Forum | Thu Jan 25 13:20:17 EST 2007 | slthomas

Are you running a lead free process? If not, have you identified these as lead free components? If so, have you increased the temps in your profile to accomodate that? After that, I'd look for a AgPd (silver/palladium) or some other such PITA platin

Same wave process do not apply to all finish board

Electronics Forum | Fri Oct 14 11:56:49 EDT 2005 | patrickbruneel

Mika, 1.) Is there a maximum board thickness where it would be almost impossible to get a decent hole fil? Answer: The thicker the board the further the solder has to travel and the more you depend on solderability of boards and components, machine

Same wave process do not apply to all finish board

Electronics Forum | Thu Oct 13 15:41:30 EDT 2005 | lyrtech

Hi, We have a customer who give us a 20K board contract each year. It's only thru-hole components.The baord is HASL plated. So we pass it into our wave. No problems. Recently, our customer decided to go into GOLD PLATED finish. We take the same re

Same wave process do not apply to all finish board

Electronics Forum | Fri Oct 14 09:58:13 EDT 2005 | patrickbruneel

Here's what I believe is happening. The main difference between the HASL boards and the gold plated boards is that HASL boards are pre-soldered. HASL boards need very little flux activity to get good hole fill and the machine settings have a wide pro


lead free solder to gold plated component searches for Companies, Equipment, Machines, Suppliers & Information

SMTAI 2024 - SMTA International

Reflow Soldering 101 Training Course
PCB Handling Machine with CE

Stencil Printing 101 Training Course
PCB Handling with CE

World's Best Reflow Oven Customizable for Unique Applications