LGA component rework process on SRT machine

Electronics Forum | Sat Jun 05 13:38:22 EDT 2021 | ppcbs

For Linear Tech LGA's we solder bump the LGA using a .30mm solder ball then reflow with a tacky flux. This will provide a void free solder joint and adds a little height to the solder joint in case you use a flux that you want to clean from under th

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Tue May 26 15:27:36 EDT 1998 | Dave F

| | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and s

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Wed May 27 21:05:30 EDT 1998 | Steve Gregory

Hey yooze guys! Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any posts f

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Tue May 26 21:27:33 EDT 1998 | Earl Moon

| | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered a

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Wed May 27 11:19:34 EDT 1998 | Earl Moon

| | | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered

Stain on PCB from reflow oven

Electronics Forum | Fri Apr 16 12:47:48 EDT 2010 | boardhouse

White solder mask does have a tendency to yellow within the lead free environment. so double coating will not help any. I due believe the flux is a factor in the yellowing but due to the color is the main reason. Find out what brand of S/M mask they

Leaded and Lead Free BGA's on hte same board

Electronics Forum | Thu May 01 15:42:53 EDT 2008 | ck_the_flip

Yes, the authors do give the caveat that small amount of lead contamination in a SAC/Lead-Free system is tolerated provided the Pb-BGA has sufficiently reflowed. This verbiage is on the bottom of Figure 10. For my own peace-of-mind, I would send yo


leaded solder on a lead free hasl pcb searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830