Re: Tin-Lead thickness on PWB's

Electronics Forum | Mon May 18 22:54:04 EDT 1998 | Dave F

.025" pitch so the only problem we run into is too much HASL on the adhesive side causing improper glue dispense. | | As Earl keeps saying HASL thickness is hard to impossible to control. I think we need to look hard at OSP's again but then you get

what is the different between ENIG and Immersion Au

Electronics Forum | Thu Jan 12 10:05:13 EST 2006 | davef

There's a lots comparisons like this on the web. Here's one: Westwood Associates said on 8/12/2003: ||HASL||OSP||ENIG||Pd||Tin||Silver Flat||no||yes||yes||yes||yes||yes Solderjoint||Cu-Sn||Cu-Sn||Ni-Sn||Ni-Sn||Cu-Sn||Cu-Sn Contact||E-test, ICT||no|

Re: HASL - again?

Electronics Forum | Mon Jun 21 09:58:25 EDT 1999 | Christopher Cross

| | Now don't everyone jump on this at once, but it seems time for me to send out copies of my not even close to being dated copy of an article about HASL. Though it was published in 1992, in Printed Circuit Fabrication Magazine, and it got rave revi

OSP Handling

Electronics Forum | Fri Jun 27 10:27:59 EDT 2003 | davef

Since you�re asking the question about proper handling of OSP board, there may still be time to talk you out of using that material. * Cleaning of mis-printed board could cause non-wetting problems. This tends to remove a fraction of OSP coating. 0.3


matte tin shelf life searches for Companies, Equipment, Machines, Suppliers & Information

Selective soldering solutions with Jade soldering machine

High Precision Fluid Dispensers
Pillarhouse USA for Selective Soldering Needs

High Throughput Reflow Oven
Software for SMT

World's Best Reflow Oven Customizable for Unique Applications