Systems for Solderability-tests

Electronics Forum | Tue Jun 25 09:31:45 EDT 2002 | Myfloh

Hi everybody, Does someone have experience in the assesment of Surface Mount devices? For the moment we have the Must System II of Multicore but it is not effective to assess the solderability of Surface mount devices. Indeed the conditions are not

Sensbey Spray Fluxer

Electronics Forum | Thu Aug 01 15:50:15 EDT 2002 | pjc

I had a 1995 SENSBEY MXL-400J at the last place I worked. I had very good results- easy to setup, run and maintain. It has a paint gun type spray head. Good idea to have spares cause they can clog. I sprayed a Multicore NC flux. Only downer was a fai

Leaching

Electronics Forum | Mon Apr 28 16:36:11 EDT 2003 | razor

Component: Termination (barrier) NI, 120/3.0 um Solder Plate (outer) 90% Sn, 10% Pb, 120/3.0 um Solder: Multicore CR39, 95.5%Sn/3.8%Ag/.7%Cu @ 6mil Flex PCB: Cu, Ni, Au .2m to .5m Thanks

fine pitch printing

Electronics Forum | Wed May 17 13:48:37 EDT 2006 | dwelch123

I'm having trouble printing leads on a fine pitch part. The lead is only .008". I'm using a DEK 265 with metal squeegee and using WS200 multicore solder paste.The stencil is laser cut and polished. I've experimented with different pressures and diffe

Palladium poor wetting

Electronics Forum | Tue May 23 09:16:57 EDT 2006 | Steve

Had exactly the same type of issues. Tried everything from pre fluxing the pcb's , various ammendements to the oven profile and various pastes. Finally after a lot of help from multicore we settled on a paste by the code of cr39. A no clean flux wit

Flux Compatibility Issues....

Electronics Forum | Tue Jun 06 12:23:54 EDT 2006 | jdumont

Thanks for the reply. I actually heard back from Kester who say they dont test with other fluxes (obviously) but that there shouldnt be any issues. Of course they recommended their wave flux to replace our Multicore and can confidently then say there

Contaminants after SMT which affect wire bonding

Electronics Forum | Fri Oct 06 04:23:06 EDT 2006 | David

What is the solder finish of the board?. If this is gold, maybe you should check the reflow profile and max temperature which can easely kill your gold coating so problems with bonding. Also we are using Prozone Multicore with ultrasonic to clean

Versaflow dross buildup

Electronics Forum | Fri Jan 25 11:49:09 EST 2008 | toddl

Hi all, I have an inconsistent situation. Lately, we seem to have excessive dross buildup in the solder pot which inturn causes the pot to overflow. Has anyone had a similar experience? Here are the details: age of machine= 9 years, flux used= Kester

wave finger cleaner solution

Electronics Forum | Tue Jul 29 22:13:59 EDT 2008 | davef

IPA is a fire hazard. Be sure your fire extinguishers are charged and your evacuation plan is current, when using IPA in the vacinity of a wave solder machine. Have you tried DI water? Solutions used in wave finger cleaners include: * Techspray SMT

Solder paste Density

Electronics Forum | Wed Aug 13 22:23:24 EDT 2008 | davef

8.4 * SAC305 => 7.36 * Sn-3.5Ag => 7.5 * '....in' [96.2Sn-2.5Ag-0.8Cu-0.5Sb] => 7.39 * Sn-4Ag-0.5Cu => 7.39, 7.44 * Sn-3.8Ag-0.7Cu (Multicore solder) => 7.5


multicore searches for Companies, Equipment, Machines, Suppliers & Information

Void Free Reflow Soldering

Best Reflow Oven
Voidless Reflow Soldering

High Throughput Reflow Oven
2024 Eptac IPC Certification Training Schedule

Wave Soldering 101 Training Course
2024 Eptac IPC Certification Training Schedule

World's Best Reflow Oven Customizable for Unique Applications