Full Site - : nickle plated bake (Page 2 of 15)

How to Prevent Solder Ball and Bridging Defects during the SMT Reflow Process

Industry News | 2018-10-18 08:32:52.0

How to Prevent Solder Ball and Bridging Defects during the SMT Reflow Process

Flason Electronic Co.,limited

Indium Corporation to Feature Precision Au-Based Die-Attach Preforms at SPIE Photonics West

Industry News | 2024-01-29 11:36:51.0

Indium Corporation® will feature its high-reliability, Au-based precision die-attach (PDA) preforms for critical laser and RF applications at SPIE Photonics West, Jan. 27-Feb. 1, in San Francisco. SPIE West is the world's premier event for lasers, biomedical optics and biophotonic technologies, quantum, and optoelectronics.

Indium Corporation

SMT Dictionary – Surface Mount Technology Acronym and Abbreviation

Industry News | 2018-12-08 03:29:29.0

SMT Dictionary – Surface Mount Technology Acronym and Abbreviation

Flason Electronic Co.,limited

JOHNSON VALVE

JOHNSON VALVE

New Equipment | Components

108038  JSNA11A-1C  CONTROL TEMPERATURE 20' CAP 96616  JSNA11B-1C  CONTROL TEMPERATURE 20' CAP 166053  JSNA19AAC-9C  DIFFERENTIAL FIXED 100/240 5F 207381  JSNA19ABA-40C  CONTROL TEMP REM BULB 104566  JSNA19ABC-24C  THERMOSTAT REMOTE BULB 98260 

zhengzhou yuzhe electronic technology co.,ltd

Soldering to nickle plated kovar parts

Electronics Forum | Tue Mar 09 21:17:10 EST 2004 | gm05688

When soldering a metalized germanimum window to a nickle plated kovar part, I would like to understand the intermetalic. Does the nickle plate actually melt or will the solder(SN63)simple stick to the nickle and not cause nickle to reflow? Any one ou

Soldering to nickle plated kovar parts

Electronics Forum | Tue Mar 09 22:26:17 EST 2004 | davef

You should to be soldering to the nickel. The intermetallic is Ni3Sn4. "At relatively low temperatures, the tin-nickel layers form about as rapidly as the tin-copper layers do, but at higher temperatures their growth rate is distinctly lower. At 10

PCB bake

Electronics Forum | Thu Jan 17 20:33:05 EST 2002 | ianchan

Hi, Can anyone help explain the benefits/disadvantages of bareboard pcb baking, as part of the pre-heat conditioning, before the bareboard pcb use in SMT production run? The pcb board is 200mm x 240mm panelized pcb board, and has 28 smaller pcb boa

Gold plated PCB's

Electronics Forum | Sun May 05 22:18:20 EDT 2002 | ianchan

Hi mate, we had a crap experience (once...no more...) with gold plated over nickle (Au/Ni) PCB that had nickle contaminents in the PCB supplier's gold bath. the Ni caused batch-delivery of the PCB to us for mass production, to exhibit the visible s

discolored pbfree finish after bake and/or reflow

Electronics Forum | Thu Apr 20 22:14:51 EDT 2006 | raquel

hello! need ur inputs... if the Matte Sn pbfree finish of the component discolors AFTER having been exposed to bake, or, after reflow, will the base leadframe have any potential contribution to it? i know most likely suspects would be the plating pro

Prob in Gold plated PCB prod

Electronics Forum | Sun Apr 11 14:35:25 EDT 2004 | davef

Please: * Describe the color and texture of the dry solder connection on the board. * Tell us the thickness of the gold and nickle plating on the board pads. * Inform us about the width and scope of the problem.


nickle plated bake searches for Companies, Equipment, Machines, Suppliers & Information