Electronics Forum | Thu Mar 25 19:29:07 EST 1999 | Graham Naisbitt
| | Hi, | | I have a customer who's electronic assemblies produce RF. He is insisting upon aqueuos cleaning. We switched to a no clean solder years ago and no longer have an aqueous system. | | Is aqueous cleaning necessary to eliminate 'cross ta
Electronics Forum | Mon Mar 29 19:31:29 EST 1999 | Scott McKee
| | | Hi, | | | I have a customer who's electronic assemblies produce RF. He is insisting upon aqueuos cleaning. We switched to a no clean solder years ago and no longer have an aqueous system. | | | Is aqueous cleaning necessary to eliminate 'cr
Electronics Forum | Tue Sep 10 22:29:01 EDT 2002 | scottefiske
Many times after initially cleaning in the solvents recommended by the paste/material manufacturer, a light white haze may still be visable...try using a soft bristle brush to remove the remaining residues. By this time the residues that remain will
Electronics Forum | Tue Sep 17 15:59:48 EDT 2002 | Randy V
No-Clean fluxes are difficult to clean off boards. Cleaning effectivness depends on the washer, the chemistry, the flux type, number of reflows, and the time between reflow and washing. White residue is flux residues that have started to break down b
Electronics Forum | Fri Aug 28 05:07:59 EDT 2009 | sachu_70
Do you clean the stencil manually or using the automated under-stencil cleaner on your Printer (recommended)? 1. Ensure that stencil wipes are lint-free and soaked sufficiently with solvent before use. 2. If your printer supports automated cleaning
Electronics Forum | Sat Jul 28 05:31:20 EDT 2001 | nop_e
Hi all I just got feedback from my customer about "White residue problem" around solder joints with manaul soldered connector at customer site and included the failure analysis report that there is residues of Cl,S,Na . I 'd like to know, the whi
Electronics Forum | Sun Jul 29 09:17:20 EDT 2001 | davef
Tough to say, but ... Chlorine: Many fluxes contain chlorine. Sulphur: Many solders and paper packing materials contain sulphur. Sodium: No idea. IPC-J-001 talks to board cleanliness and specifies criteria according to the cleanliness test met
Electronics Forum | Tue Jan 30 18:25:25 EST 2018 | aqueous
This is one of the most common questions I get asked. Why clean no-clean flux. It was stated earlier that no-clean residues are benign. This may or may not be accurate. It depends on several factors including the reflow process. In a perfect world, t
Electronics Forum | Thu Feb 01 17:34:45 EST 2018 | Mike Konrad
Thanks for the kind words Dave. At no point in my reply was I trying to sell anything. I apologize to anyone who believes otherwise. I agree with the poster, if assemblies are going to be cleaned, consider a flux designed to be cleaned. While this is
Electronics Forum | Tue Jan 30 07:29:21 EST 2018 | charliedci
I believe the correct statement (I've been told) is "the process is no clean". The solder paste is "low residue". As a CM, in the past we had customers that insisted on a wash after soldering. We used DI water with a saponifier which had mixed result