Electronics Forum | Tue Oct 24 09:35:56 EDT 2000 | Wister
Our important customer demanded us to use 12mil thick stencil,it is too difficult to release solder paste from stencil.it is not helpful even I ask stencil supplier polished the openings.The flux content is 10%. I want to ask if the polyurethane sque
Electronics Forum | Sun Sep 26 21:41:36 EDT 2004 | mark_h
Hi All Thanks for your interesting replies :) At this stage I feel that we are leaning towards a second hand DEK 265 GSX vs a new EKRA E4 or X4, and with the saving made we will get it well refurbish and add a board loader, and hopefully a proflow
Electronics Forum | Thu Jul 28 07:23:24 EDT 2011 | scottp
My group supports a couple hundred lines all over the world. Most of them use squeegees but a few use either the MPM Rheometric pump heads or the DEK Proflow heads. I absolutely hate the enclosed heads. Flux separation, compaction, and the print q
Electronics Forum | Tue Aug 22 12:14:21 EDT 2000 | Tekguy2000
There are concretions that form inside the chamber when using a water soluble paste. They start forming and affecting print as early as 2 days. This is apparent no matter what type of print head you may be using. There has been over 30 water soluble
Electronics Forum | Wed Aug 30 08:06:45 EDT 2006 | scombs
The reason I asked earlier about Gridlok is that we are using the on 2 Dek Horizon printers (since Jan 06) with edge clamps and they work well. We run them in Auto mode so they conform to the board at each print so I do not have to worry about the op
Electronics Forum | Wed Aug 27 11:06:30 EDT 2003 | Rich A.
Anyone experience of using Water Soluble paste in pump printing heads, either Dek proflow or Rheopump. Thanks in advance, RA.
Electronics Forum | Tue Sep 07 15:28:13 EDT 1999 | Earl Moon
Listed below are the issues Viking has been experiencing since the installation of the Proflow Head: 1. After installing new 350mm Wiper foil with metal strip glued on it, It worked for about a week and suddenly metal stri
Electronics Forum | Wed Sep 08 08:25:26 EDT 1999 | Brad Kendall
Listed below are the issues Viking has been experiencing since the | installation of the Proflow Head: | 1. After installing new 350mm Wiper foil with metal | strip glued on it, It worked for about a week and suddenly meta
Electronics Forum | Fri Aug 18 09:19:01 EDT 2000 | PR
We have been using the Pro Flo for about a year and the print quality alone is worth making the move. It is flexible in that switching over to blades is pretty simple (if you need to), and the operators love it because clean up is a breeze. The only
Electronics Forum | Sat Nov 15 05:08:45 EST 2014 | grimus
Same side (component side) if You give me e-mail I can provide You more pictures. I'm making one stroke with same speed (I'm using closed proflow head and DEK printer). 5 mils thickness stencil. Products requirement - 3 IPC Class (75 % and more fill