Electronics Forum | Tue Sep 03 17:48:34 EDT 2002 | dphilbrick
My customer is finding a blue haze on some SMT pads after processing, kind of looks like a water spot on the surface of solder joints. It requires 20x mag and very good lighting to see. We have done 2 different ionic tests and the boards pass to clas
Electronics Forum | Tue Jul 15 18:44:20 EDT 2003 | davef
Sam says, �The only question remaining to me is that why the failure happened after 48 hours instead of immediate failure after soldering.� Let�s recap: * Had good-looking solder flow. * Passed the initial electrical test. * Failed the later electri
Electronics Forum | Thu Jun 25 14:45:55 EDT 1998 | Chrys
| I have a single-sided board with test vias that pass through the board. The test vias are pasted and reflowed with the SMT components on the top side. When the boards are wavesoldered, the solder coverage on the vias is spotty. Some will sold