Electronics Forum | Fri Oct 26 17:01:52 EDT 2001 | davef
We process no Teflon boards. Companies, such as Rogers and Taconic, make laminates of Polytetrafluoroethylene [PTFE] er �Teflon�. Common �Teflon� laminates are: * Woven glass / PTFE * Random microfiber glass / PTFE * Ceramic / PTFE * Woven glass /
Electronics Forum | Mon Jul 01 20:45:38 EDT 2002 | davef
Solder mask thickness specifications by fabricators are: * Wet mask: 0.0002 ~ 0.0004� on trace * LPI mask: 0.0002 ~ 0.0008� on trace Liquids usually range between 10 to 13 um (0.00039 to 0.00051") when dried. Liquid resist processes I have seen are
Electronics Forum | Wed Apr 09 20:05:21 EDT 2003 | davef
Kevin: We know of no handy approach to developing recipes. * Certainly programs provided by profiler suppliers give you a good first pass, based on your oven and solder paste. * Second pass in developing your recipe comes through trail and error chan
Electronics Forum | Wed May 07 09:31:28 EDT 2003 | davef
We use uV Dymax glue for thermocouple attach sometimes, but don't like the remainder [anal] and loosing attach, sometimes. Roger Saunders, President Saunders Technology, Inc; said: PRO: � These products are easier to use than high temperature solde
Electronics Forum | Fri Apr 30 08:28:39 EDT 2004 | davef
Roger Saunders, President Saunders Technology, Inc wrote a fairly unbiased paper that compared different thermocouple attach methods. You can probably find it on their site. In it, about gluing thermocouples, he says: There are two general classes
Electronics Forum | Tue Jan 16 20:34:17 EST 2007 | davef
DAVE�S BOOKSHELF ASSEMBLER�S ESSENTIALS Title: Soldering in ElectronicsAuthor: RJ Klein WassinkPublisher: Electrochemical PublicationsISBN: 090115024XPublication date: December 1989 I know, I know. The book was written in 1989!!!! I use this b