Industry News | 2013-09-14 09:00:12.0
Essemtec will exhibit in booth #827 at the upcoming SMTA International Exhibition, scheduled to take place October 15-16, 2013 at the Fort Worth Convention Center in Texas.
Industry News | 2020-12-03 13:07:26.0
Indium Corporation's newest jetting and microdispensing solder paste, Indium12.8HF, has been officially recommended by NSWAutomation for use with their newest microfluid dispenser, SD1.
Industry News | 2024-03-18 11:39:20.0
We are showcasing our flagship All-in-One platforms FOX and PUMA. The machines will be equipped with the latest innovations in Solder Jetting, Integrated Inspection System, Smart Material Management, and 4 mm EVO feeder – 08004 Pick-and-Place.
For everything from high volume, low cost capacitors to application specific ceramic solutions, Johanson Dielectrics has you covered. The mission of the Johanson Companies is to translate our customer needs into quality electronic components, produ
Industry News | 2019-11-05 22:10:56.0
Many customers and electronic designers were asking questions about the aluminum-based board, today our chief technical official Luca Zhang shared the knowledge and experience to you.
Industry News | 2018-12-08 03:29:29.0
SMT Dictionary – Surface Mount Technology Acronym and Abbreviation
Electronics Forum | Thu Aug 12 20:32:44 EDT 2004 | usdigital
Indy, We use Palladium silver surface finish parts for silver epoxy attached parts only. It is our understanding that this finish is not for solder, but only silver epoxy attach. I expect that is you problem. Dave
Electronics Forum | Thu Apr 29 18:48:11 EDT 1999 | Kiet Dang
Hi, Did anyone experience a problem with electrically conductive silver filled epoxy is resistive due to galvanic reaction? I'm having this problem when attaching components to Ni plated housing while conducting an experiment to cost reduction for Au
Electronics Forum | Sun Jul 04 19:49:05 EDT 2004 | indy
Hello Everyone, We are having some problem with Palladium-Silver surface finish. We have ceramic components with the above surface finish. When we try to assemble these on Sn/Pb solder, we are observing open joints. If we reflow the compt for more t