New Equipment | Solder Materials
Ceasolder-PAL (Pink Acrylic Latex) Peelable Acrylic Latex Solder Mask Ceasolder-Pal is a temporary, peelable solder mask comprised of a thixotropic, synthetic acrylic latex designed to withstand fluxing, wave soldering and cleaning operations. Unli
Industry News | 2011-04-06 13:13:52.0
Dow Electronic Materials will showcase its innovative materials for printed circuit boards (PCBs) at this year’s IPC APEX EXPO. Dow will feature a number of its latest products that are tailored to meet the requirements of increasingly complex circuit boards while delivering ever-higher reliability and consistency. Dow’s next-generation of high quality, cost-effective technologies allow customers to meet future market requirements.
Industry News | 2012-11-26 14:04:53.0
The IDTechEx report The Market for Gold Inks 2013-2019 is looking to identify and assess the opportunities for a printable nano-gold ink, excluding its use in graphic arts applications (where it could be used for both its graphic arts benefits in addition to being used as a functional component in a circuit, such as printed touch switches, are taken into account). Save 25% online by quoting REP2012.
Industry News | 2021-01-21 08:09:52.0
Indium Corporation announces that it is now offering CW-232,a uniquely formulated flux-cored wire that combines superior wetting speed and spread with extremely low-spatter performance.
Industry News | 2021-02-25 13:23:32.0
Indium Corporation will feature its uniquely formulated flux-cored wire during the virtual IPC APEX Expo, to be held March 8-12.
Industry News | 2018-10-18 11:08:03.0
Different Techniques for Plating
Electronics Forum | Fri Aug 30 11:53:12 EDT 2002 | genny
Possibly this is tarnish? Silver finish requires a bit more care in handling or packaging - to avoid contact with sulphur which may cause tarnish. Some cardboard boxes gas out enough sulphur to cause a problem. Possibly look at your method of stora
Electronics Forum | Fri Aug 30 16:25:21 EDT 2002 | davef
Imm silver holds-up to multiple thermal cycles very well. The things, we guess, are happening to make imm silver tough to solder after heating and sitting are: * Oxidation of the silver. * Reduction of the co-deposited organic anti-tarnish [used in
Electronics Forum | Sun Sep 08 19:58:57 EDT 2002 | dasal
My specialty. Your right, Most corrugated contains S02 and the pallet is usually out gassing formic acid as well. Not a great environment for silver. Original press release follows: Reactive Polymers At AT&T Bell Labs, John P. Franey has developed
Electronics Forum | Sun Sep 21 10:55:52 EDT 2008 | vladig
As long as the surface is solderable, you should be fine. Silver tarnish a well0-known thing. Make sure, though, there is no sulfur (S) "around". Regards, Vlad