Electronics Forum | Wed Sep 12 16:15:28 EDT 2007 | rpadilla
Does anyone have Data/Comparisons showing which component plating is better, Nickle plating vs. Sucoplate for SMT production? These components would be reflowed with a SAC305 alloy
Electronics Forum | Wed Jan 18 17:07:32 EST 2006 | gregoryyork
Sorry Bob Could not respond been away busy. Just to correct you, we did not copy the SACX as we brought ours to market at least six months before so how could we copy, it is also a little different, but nicely reassuring when the 'big boys' do some
Electronics Forum | Wed Sep 24 19:18:53 EDT 2008 | ratsalad
We had a PCB vendor provide us with SAC105 plated HASL boards. They worked fine on the first pass through reflow. The second pass was not pretty. We couldn't get much of anything to solder to the board. That may not have been the alloy, it could