BEST Inc master instructor Norman Mier demonstrates how to replate gold fingers using the BEST gold contact replating kit. In this video he demonstrates how to repair, prepare and replate the finger using a gold replating solution. If you want to lea
This video presents the capabilities of BEST Inc in terms of its ability to perform high end PCB rework and repair services. BEST Inc., located in Rolling Meadows IL is a company of soldering "geeks". We rework/repair PCBs, train and certify solderin
New Equipment | Rework & Repair Equipment
The BEST Gold Contact Replating Kit includes the tools you need for fast replating and modification of circuit contacts. Edge contacts may require replating if they are contaminated with solder or become scratched during handling or do not meet the m
New Equipment | Solder Paste Stencils
Eliminate hours of solder mask damage repair time for bga sites while improving rework yield. Are you frustrated by the time it takes to repair mask damage underneath the BGA during the rework process? Are you squeezed for space on the PCB in an
StencilQuik demonstration video. This breakthrough method allows you to simplify placement/replacement saving 50% or more of time required to rework BGAs or CSPs.This is a well developed BGA rework method. More on the StencilQuik(TM) process here:
SMT contact fingers The SMT contact fingers are ideal for automatic placement and can be delivered on Tape and Reel packing. When the contacts are mounted in a row they can provide excellent RFI shielding connection for metal doors or other cabinet
Industry News | 2019-05-16 01:27:23.0
There are several surface treatment for PCB board: bare board (no treatment on the surface), rosin board, OSP (Organic Solderability Preservatives), HASL (lead tin, lead-free tin), plating gold, immersion gold, etc., these are relatively conscious treatment. Many people can't tell the difference between plating gold and immersion gold, thinking that it is the same thing, it is a big mistake. The following is a brief introduction to the difference between plating gold and immersion gold.
Layer: 10L Base Material:FR-4 tg180(ITEQ) Board Thickness: 1.6mm Final copper: 35um Surface Finish:Immersion Gold/Au:2u” min. Gold fingers/Au:30u” Solder mask: Green Profile: Routing E-test: 100% Fixture Quality report: Solderability test, Fi
New Equipment | Fabrication Services
Our Service PCB Assembly and PCB&PCBA design are our main business.We are able to undertake a high quality Printed Circuit Board Assembly on competitive prices and flexible conditions.We are a complete “One- Stop” resource for printed circuit board
New Equipment | Solder Materials
Solder pallet made from durostone composite material The material: Solder pallet is made from Durostone anti-static black composite material and reinforced fiberglass. The product uses a high performance glass-filler for improved ma