Electronics Forum | Thu May 18 16:27:53 EDT 2006 | bman
I don't have any experinence with this, but my concern is that you are limiting the amount of contamination your pot can absorb before you ever run a board through. What I mean is that even if you are able to drain all but about a kg of the old sold
Electronics Forum | Thu Dec 10 05:58:59 EST 2009 | gregoryyork
Best to use Tin treated with TinP Additive. This ensures the Tin is fluid enough to Dissolve any Leaded residues. Run the machine for one hour at 275C then take out wave former and as much of the workings of the pot as possible. Then start bailing ou
Parts & Supplies | Soldering - Wave
Titanium solder pot liner for a Vectra 450F solder pot. Converting your wave solder to Pb Free? Use a titanium solder pot liner to avoid the costly tin flush and risk of contamination. FOB: Origiin Contact: Assured Technical Service LLC AssuredT
Surface Mount Technology Association (SMTA) | https://www.smta.org/icsr/speaker_forms/Paper-Format-Requirements.doc
· All body text - 10pt. Times New Roman or equivalent ‘serif font’ · Justify / block text - no indents for paragraphs · HEADINGS - flush left
GPD Global | https://www.gpd-global.com/co_website/pdf/lead-former/CF8-Doc-Package-801-1-01.pdf
5.3.2.1 Horizontal Flush-Mount Form Calculations . . . . . . . . . 5-9 5.3.2.2 Horizontal Stand-Off Form Calculations . . . . . . . . . . 5-10 5.3.2.3 Vertical Flush-Mount Form Calculations