Tomb-Stoning. What's going on here?

Electronics Forum | Wed Jan 18 10:35:17 EST 2006 | pms

Thanks folks !! I'll experiment with the bottom side heaters. Unfortunatly I don't think our Vitronics-Soltec oven has the option for adjusting the heater fan speeds. And I'll check the conveyor chains. This is our first project using 0402 parts, wh

Midchip solderballs (MCSB) on pb-free

Electronics Forum | Tue Sep 26 12:01:30 EDT 2006 | sliebl

We have solved our MCSB problems by using standard homeplate designs on all of our resistors and caps. I use a 50% taper and have achieved great results with 0402-1206 parts using both tin/lead and SAC305 paste. We use Amtech paste.

Re: 0603's on 0805 pads

Electronics Forum | Mon Aug 28 18:57:41 EDT 2000 | Earl Moon

Steve, This is a good, well repeated, not identified by IPC yet issue. I, and some others in industry, for years have proven and recommended smaller pads for various devices. I, and some others in industry, use 0402 pads for 0603 device types. IPC o

Solder balls on Cleaned process

Electronics Forum | Wed Oct 17 13:02:41 EDT 2001 | Yngwie

We are running Clean process. solder beadings were found after the wash process. Weird eh!! It's true.. Details: 1)wash pressure ? No shadowing effects from high profile component. It also happened on the component's body of the 1210 & 0402 caps whi

Re: Wierd Tombstoning on Tant Caps

Electronics Forum | Sat May 02 00:51:14 EDT 1998 | Rick

I agree with Steve...most certainly a placement occurance. I've seen this on many occasions with Panasonic equip. Change your feeder first and then check your component packaging. | I've never seen this before. Today, I got this tombstoning on Tan

Re: Wierd Tombstoning on Tant Caps

Electronics Forum | Mon May 04 21:54:14 EDT 1998 | Dave F

| I've never seen this before. Today, I got this tombstoning on Tantalum Capacitors (Okay, I saw that before) | Here's the part that seems weird to me: | -They didn't tombstone onto a termination - they went onto their sides! That's right, both ter

Re: Wierd Tombstoning on Tant Caps

Electronics Forum | Fri May 01 22:05:23 EDT 1998 | D.Lange

| I've never seen this before. Today, I got this tombstoning on Tantalum Capacitors (Okay, I saw that before) | Here's the part that seems weird to me: | -They didn't tombstone onto a termination - they went onto their sides! That's right, both ter

Re: Wierd Tombstoning on Tant Caps

Electronics Forum | Fri May 01 14:44:26 EDT 1998 | Earl Moon

| I've never seen this before. Today, I got this tombstoning on Tantalum Capacitors (Okay, I saw that before) | Here's the part that seems weird to me: | -They didn't tombstone onto a termination - they went onto their sides! That's right, both ter

Re: Wierd Tombstoning on Tant Caps

Electronics Forum | Mon May 04 12:07:58 EDT 1998 | ETS, LLC

As an employee of a Reflow Oven Manufacturer I can only make suggestions on the oven portion of your process: As I was reading through your posting I started wondering if you are using a convection or IR based oven. If you are using Convection I woul

Re: Wierd Tombstoning on Tant Caps

Electronics Forum | Fri May 01 20:12:29 EDT 1998 | Steve Gregory

| I've never seen this before. Today, I got this tombstoning on Tantalum Capacitors (Okay, I saw that before) | Here's the part that seems weird to me: | -They didn't tombstone onto a termination - they went onto their sides! That's right, both ter


tombstoning on 0402 caps searches for Companies, Equipment, Machines, Suppliers & Information

Count On Tools, Inc.
Count On Tools, Inc.

COT specializes in high quality SMT nozzles and consumables for pick and place machines. We provide special engineering design service of custom nozzles for those unique and odd components.

Manufacturer

2481 Hilton Drive
Gainesville, GA USA

Phone: (770) 538-0411