Electronics Forum | Thu Dec 22 15:36:03 EST 2005 | CC
In general two step temperature reflow process requires minimum 40 deg C delta to be sucessful. We are not using vapor phase soldering but we have similar situation when we change to SAC lead free solder for PCB component population and secondary swe
Electronics Forum | Thu Dec 22 12:05:37 EST 2005 | Tony
Currently we are using a 2 step vapor soldering process to manufacture our std. lead soldered parts. The first step was done with a ls240 vapor fluid and the second was done with a ls200 fluid. Using a 221 deg C sn95/Ag5 solder for the first step a
Electronics Forum | Mon Jul 19 12:37:15 EDT 1999 | Wolfgang Busko
| | | | | Hi, SMTASSY | | | | that�s what we do, soldering our double-sided-finepitch-BGA-and all-the-other-stuff-boards in vapourphase because it�s the only thing we have. | | First, we do not do real series produktion, only prototyping up to som
Electronics Forum | Tue Jul 20 05:29:14 EDT 1999 | Wolfgang Busko
| | | | | | | | Hi, SMTASSY | | | | | | that�s what we do, soldering our double-sided-finepitch-BGA-and all-the-other-stuff-boards in vapourphase because it�s the only thing we have. | | | First, we do not do real series produktion, only prototypi
Electronics Forum | Wed Sep 17 04:15:23 EDT 2003 | C Miller
The magnetic thing from the sot23 thread made me think of somthing from the past. Does anyone have any experience with vibrating boards during reflow? I know for a fact that if you vibrate a board during reflow it will alow the parts to "float" and
Electronics Forum | Fri Mar 21 20:21:41 EST 2003 | Grant
Hi, I can verify that, and we have done 2 or more reflows with prototypes, using vapor phase reflow, and because there is no oxygen, the result is good, and you cannot tell the difference between the first reflow, and the 3rd. We are getting a vap
Electronics Forum | Wed Mar 19 20:40:27 EST 2003 | arminski
Vapor Phase process can do reflow from 4 to 5 times!
Electronics Forum | Fri Mar 29 11:02:04 EDT 2019 | robl
Not sure it's always a great route as the smaller ovens are going to struggle to get a perfect profile for a consistent result, especially on bigger boards with higher layer counts and mixed technology. You may want to take a quick look at a batch va
Electronics Forum | Wed Jan 30 12:37:49 EST 2002 | jax
nifhail, In a nutshell: Vapor-phase reflow is a process that uses a fluid with a selected boiling point. As condensation of the hot vapor occurs on a cool assembly the assembly's temperature is rapidly raised to match the temperature of the vapor.
Electronics Forum | Tue May 23 14:02:47 EDT 2006 | patrickbruneel
Stephen, you better believe the nurse she's right If it would be possible to produce lead vapors you would see lead vapor condensation in the hood or in the ducts. Never seen any lead deposits anywhere. There is no reason for concern The absence of