BGA bake out....

Electronics Forum | Mon Jun 28 09:15:21 EDT 2004 | jdumont

Morning all, we have been seeing some problems with the edges of some of our BGA's curling away from the PCB after reflow. Is this possibly a moisture problem? If so what would be a good time/temp to bake them at to rectify the problem? Thanks in

Baking assemblies after ultrasonic water wash

Electronics Forum | Wed Jun 10 22:47:17 EDT 2009 | davef

You're correct that JEDEC J-STD-033 defines baking condidtions for moisture sensitive components. Why do you want to bake assemblies after cleaning? Search the fine SMTnet Archives for threads like: http://www.smtnet.com/forums/Index.cfm?CFApp=1&Me

Baking assemblies after ultrasonic water wash

Electronics Forum | Wed Jun 24 05:08:37 EDT 2009 | Mark

Try immersing the assembly in IPA for 30 minutes. IPA is hydroscopic ans will drive off most of the water. Dry the assembly. Then bake at 110°C for 2 hours.

Baking assemblies after ultrasonic water wash

Electronics Forum | Tue Jun 09 18:44:20 EDT 2009 | dyoungquist

We are using a water soluble flux which requires the assemblies to be cleaned in an ultra sonic cleaner after assembly. Is there a standard that specifies how long the assemblies need to be baked/dried after being submersed in a water solution for a

Baking assemblies after ultrasonic water wash

Electronics Forum | Fri Jun 26 00:28:43 EDT 2009 | Mark

IPA is hydroscopic.

Baking assemblies after ultrasonic water wash

Electronics Forum | Tue Jun 30 13:20:10 EDT 2009 | charliedci

He wants to "see underwater"

Baking assemblies after ultrasonic water wash

Electronics Forum | Thu Jun 11 10:02:36 EDT 2009 | dyoungquist

Our cleaning process involves the assemblies being completely immersed in the water bath of the ultrasonic cleaner. The assembly has a QFP44 on it. Customer stated that when these assemblies have been cleaned with water in the past (at a different

Baking assemblies after ultrasonic water wash

Electronics Forum | Thu Jun 25 20:01:54 EDT 2009 | davef

Shanelo Technologies Given that isopropyl alcohol [IPA] is produced by combining water and propene. How does soaking a board in water and a flammable liquid drive off water?

Baking assemblies after ultrasonic water wash

Electronics Forum | Wed Jul 01 05:26:31 EDT 2009 | kpm135

But the boards and parts on the boards are also hygroscopic(no not a typo I did a search on hydroscopic and it is not a word the actual word is hygroscopic look it up if you don't believe me) so if you have two hygroscopic materials which one wins?

caps have yellow stain after wash

Electronics Forum | Wed Jun 15 10:38:41 EDT 2016 | laynefelix

Hi everyone..i am new here. I am hardware design engineer and as per my experience PCBAs came out cold soldered after being reflowed the first time with ALPHA WS-820. The flux gel ALPHA WS 609 was supposed to be applied only onto the terminations of


wash pcb after bake searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830

Global manufacturing solutions provider

High Precision Fluid Dispensers
Blackfox IPC Training & Certification

Wave Soldering 101 Training Course
SMT feeders

Best Reflow Oven
Selective soldering solutions with Jade soldering machine

Training online, at your facility, or at one of our worldwide training centers"
Best SMT Reflow Oven

World's Best Reflow Oven Customizable for Unique Applications


"回流焊炉"