Electronics Forum | Thu Apr 16 13:47:36 EDT 1998 | Lou
| We are having some difficulty soldering a 240 pin Altera device. We use Alpha WS-609, a very generic profile for that solder paste, and a 6 mil stencil with laser cut apertures (1:1 ratio). This is a 20 mil pitch device (aperture size is 10 mils X
Electronics Forum | Thu Sep 03 04:53:31 EDT 2009 | d0min0
to summarize - 3 components are placed on a single module x 8 on pcb - 2 anodes & 1 cathode are infected (so no component for us) - the problem does not look like wetting problem as the component and land pad is wetted, but the paste is not complete
Electronics Forum | Sun Dec 10 11:55:16 EST 2000 | Bob Willis
The following may be of interest to you. INTRODUCTION TO X-RAY INSPECTION All text Copyright Bob Willis, EPS INTRODUCTION TO X-RAY INSPECTION The use of X-ray inspection is becoming very popular due to the increased use of Ball Grid Array (BGA)
Electronics Forum | Sun Dec 10 11:55:28 EST 2000 | Bob Willis
The following may be of interest to you. INTRODUCTION TO X-RAY INSPECTION All text Copyright Bob Willis, EPS INTRODUCTION TO X-RAY INSPECTION The use of X-ray inspection is becoming very popular due to the increased use of Ball Grid Array (BGA)
Electronics Forum | Sun Dec 10 11:56:05 EST 2000 | Bob Willis
The following may be of interest to you. INTRODUCTION TO X-RAY INSPECTION All text Copyright Bob Willis, EPS INTRODUCTION TO X-RAY INSPECTION The use of X-ray inspection is becoming very popular due to the increased use of Ball Grid Array (BGA)
Electronics Forum | Thu May 17 07:36:40 EDT 2001 | Bob Willis
Here is a copy of a draft document on PIHR Inspection I have jotted down on a flight to Scotland yesterday, any comments suggestions etc ? I have already most of the photos for the standard but as you know there is nothing in the IPC document it just
Electronics Forum | Sat Feb 12 09:08:47 EST 2000 | Sal
Experiencing a problem with a 208 PBGA device. I am achieving good wetting with the exception of one ( damn) pin on the outer corner.I have a really good profile but the worrying thing is that it is so inconsistant. Once this open pin failure is dete
Electronics Forum | Thu Jan 27 14:49:53 EST 2000 | Glenn Robertson
Tuan - One of the reasons I suggested pre-tinning (aside from the negative effects of Gold on appearance and reliability) is the known slower wetting of Sn/Ag and Sn/Cu alloys as compared to Sn/Pb. If you don't have to be Lead-free, the high Lead
Electronics Forum | Fri Jun 18 15:39:47 EDT 1999 | Earl Moon
| What's wrong with the Tin? Just wondering | | MDCox | | | | Electroless silver had promise, from Alpha, but I don't know where this ended up. Also Omikron's "white" electroless tin is proported to be a good alternative, though I've never been a
Electronics Forum | Mon Dec 18 16:13:15 EST 2006 | darby
AJ, No overprint. We have components in very close proximity that precluded that. Also we have differing areas of thermal relief for the pads from a large backplane, from none at all to open blocks to individual pad relief. After a few more experimen