Industry Directory | Consultant / Service Provider
Winslow Automation has been advancing lead finish and soldering technology for the military and aeropace, telecommunications, medical, and consumer electronics industry since its inception in 1986.
Industry Directory | Consultant / Service Provider / Manufacturer
U.S. based contract manufacturer providing turn-key EMS solutions to defense and commercial OEM's.
New Equipment | Education/Training
The areas in which we are conducting research comprise a comprehensive group of inter-related issues and concerns involving all military, industrial and commercial electronics users facing conversion to lead free solder alloys. REI’s DoD currently
New Equipment | Assembly Services
Perfectly Controlled Immersion Tin System The Horizon Stannatech system is the leading immersion tin system within the entire PCB industry. Together with the Stannatech process and Atotech's unique Crystallizer and ConStannic control systems for im
Electronics Forum | Sat Dec 10 08:13:53 EST 2005 | davef
We believe imm tin suppliers say that their product does not whiskey, oops whisker, because they use 'white tin' not the 'gray tin' that causes whiskers. But as soon as you alloy their tin with SAC or any other high tin content solder, all bets are
Electronics Forum | Mon Dec 12 13:09:46 EST 2005 | Kris
do you intend to use Immersion tin as a PCB surface finish ? Then Whisker concern is as below if you do not past your test pads, the pads will be stressed when probed on a ICT or a flying probe tester. This is a POTENTIAL for whiskers There is a lo
Industry News | 2003-06-23 08:49:39.0
Three Organizations from the US, Europe and Japan to
Industry News | 2012-03-26 15:58:58.0
Tin whisker growth, risk mitigation, detection and failure analysis will be the focus of the IPC Tin Whiskers Conference, April 17–19, 2012, in Ft. Worth, Texas.
Technical Library | 2019-06-19 11:06:46.0
Tin (Sn) metal displays the characteristic of growing “tin whiskers” from pure tin coatings (most actively on relatively thin, electrodeposited or immersion tin coatings), usually months or years from the initial deposition of the tin. Tin whiskers are electrically conductive, filamentary, single crystals of white (beta phase) tin. These filaments of single crystal tin are usually one to five microns in diameter, and a few microns up to several tens of millimeters long, that grow spontaneously from the tin coatings. Alloying additions of several percent (by weight) of lead (Pb) prevents these electrically conductive tin whiskers from growing. Pb alloyed into the Sn was discovered to prevent the occurrence of tin whiskers in electronic assemblies in the 1950s as the Bell Laboratories solution to the problem of tin whiskers. The alloying of the tin with lead has thus quietly averted incalculable losses from short circuits in electronic equipment for the last 60 years.
Technical Library | 2019-06-20 07:45:19.0
One of the two basic risks of employing the commercially accepted, Restriction of Hazardous Substances (RoHS) compliant, lead-free (Pb-free) electronics is the threat to the electronics reliability from the growth of tin whiskers. The other basic risk deals with Pb-free solder joint reliability.
https://www.ascen.ltd/Products/conformal_coating_equipment//580.html PCB Conformal coating machine is used to paint conformal coating onto full LED panel to avoid PCB moisture,sault and static.It can be full panel conformal coating or selective coati
SN100C P810 D4????????? ???????????? ??????????????????????????????????? ?????????????? ???http://www.nihonsuperior.co.jp/
Training Courses | | | PCB Assembly Courses
The PCB assembly courses provide knowledge of different processes and equipment used in TH and SMT assembly of printed circuit boards.
Events Calendar | Thu May 17 00:00:00 EDT 2018 - Fri May 18 00:00:00 EDT 2018 | ,
Tin Whisker - All You Should Know - SMTA Webtorial
Events Calendar | Mon Apr 23 00:00:00 EDT 2018 - Thu Apr 26 00:00:00 EDT 2018 | Shanghai, China
SMTA China East Conference 2018
Effects of Tin and Copper Nanotexturization on Tin Whisker Formation SMTnet Express August 17, 2012, Subscribers: 25395, Members: Companies: 8952, Users: 33485 Effects of Tin and Copper Nanotexturization on Tin Whisker Formation First published
An Investigation of Whisker Growth on Tin Coated Wire and Braid SMTnet Express August 2, 2012, Subscribers: 25335, Members: Companies: 8941, Users: 33403 An Investigation of Whisker Growth on Tin Coated Wire and Braid First published in the 2012
Surface Mount Technology Association (SMTA) | https://www.smta.org/smtai/call_for_papers.cfm
) Tin Whiskers Wafer Level Packaging (WLP) Assembly: 01005/03015 Components/Assembly 3D Board Assembly Additive Manufacturing SMT Adhesives Alternate Solder Alloys BGA/CSP Assembly Bottom Terminated Components Cavity Board Assembly Cleaning, Conformal